Magnetic material and method for producing the same
AssigneeDaihatsu Motor Co., Ltd.
InventorsKousaku Okamura, Kazuhiko Madokoro
Life of this patent
Estimating the term…
Abstract
A magnetic material is produced by mixing a magnet powder with an amorphous metal containing a rare-earth element, iron, and boron, the rare-earth element being in the range of 22 to 44 atomic %, and the boron being in the range of 6 to 28 atomic %; and heating the mixture to a temperature or more, the temperature being lower than the crystallization temperature of the amorphous metal by 30° C., or when the amorphous metal is a metallic glass, to a temperature of the glass transition temperature thereof or more.
Claims5
A magnetic material in which a magnet powder and an amorphous metal are used as ingredients,
- wherein the amorphous metal contains a rare-earth element, iron, and boron;
- the amorphous metal contains the rare-earth element in the range of 22 to 44 atomic %, and the boron in the range of 6 to 28 atomic %;
- and
- the magnetic material is obtained by
- mixing the magnet powder and the amorphous metal, and
- heating the mixture to a temperature or more, the temperature being lower than the crystallization temperature (Tx) of the amorphous metal by 30° C., or
- when the amorphous metal is a metallic glass, heating the mixture to a temperature of the glass transition temperature (Tg) thereof or more.
A method for producing a magnetic material comprising:
- mixing a magnet powder with an amorphous metal having an initial softening temperature of 600° C. or less, thereby producing a powder mixture;
- charging the powder mixture to a mold, and pressure molding the powder mixture in a magnetic field, thereby producing a compact, and
- subjecting the compact to spark plasma sintering in the same mold, thereby heating the compact to a temperature of the initial softening temperature or more of the amorphous metal.
Dependencies are inferred from the claim text.