Elastomer Resins, Fibers And Fabrics Thereof, And Uses Thereof
AssigneeLubrizol Advanced Materials, Inc.
InventorsRavi R. Vedula, James E. Bryson, JR., Mouh-Wahng Lee, Daniel M. Fischer, Christopher A. Sprague
Life of this patent
Estimating the term…
Abstract
The present invention relates to elastomeric resins, fibers made from said resins, fabrics made with said fibers, and applications and uses for the resins, fibers and fabrics. The elastomer resins of the invention provide high strength fibers and well balanced fabrics with good physical properties and chemical resistance, making them attractive for use in various applications that use elastic fibers and fabrics.
Claims19
An elastomer resin prepared by reacting:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000.
A method of making an elastomer resin comprising the steps of:
- I. reacting in an internal mixing device:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000;
- resulting in an elastomer resin.
A method of making a fiber, film, or hose comprising the steps of:
- I. preparing an elastomer resin in an internal mixing device wherein said elastomer resin is prepared by reacting:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000;
- II. further reacting the resin composition with
- (iv) an agent comprising the reaction product of a polyalkylene ether glycol and a diisocyanate;
- and
- III. processing said elastomer resin into a fiber, film, or hose wherein said fiber, film, or hose has a weight average molecular weight of at least 700,000.
A method of making a fabric comprising the steps of:
- I. preparing an elastomer resin in an internal mixing device wherein said elastomer resin is prepared by reacting:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000;
- and
- II. further reacting the resin composition with
- (iv) an agent comprising the reaction product of a polyalkylene ether glycol and a diisocyanate;
- and
- III. melt-spinning said elastomer resin into a fiber wherein said fiber has a weight average molecular weight of at least 700,000.
- IV. processing said fiber, optionally in combination with one or more other fibers, into a fabric.
A method of improving the solvent resistance of an article, wherein said article comprises a fabric and wherein said fabric is comprised of fibers, said method comprising the steps of:
- I. preparing an elastomer resin in an internal mixing device wherein said elastomer resin is prepared by reacting:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000;
- and
- II. further reacting the resin composition with
- (iv) an agent comprising the reaction product of a polyalkylene ether glycol and a diisocyanate;
- and
- III. melt-spinning said elastomer resin into a fiber wherein said fiber has a weight average molecular weight of at least 700,000.
- IV. processing said fiber, optionally in combination with one or more other fibers, into a fabric;
- V. processing said fabric into said article;
- resulting in an article with improved solvent resistance.
A method of improving the alkali and chlorine resistance of an article, wherein said article comprises a fabric and wherein said fabric is comprised of fibers, said method comprising the steps of:
- I. preparing an elastomer resin in an internal mixing device wherein said elastomer resin is prepared by reacting:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000;
- and
- II. further reacting the resin composition with
- (iv) an agent comprising the reaction product of a polyalkylene ether glycol and a diisocyanate;
- and
- III. melt-spinning said elastomer resin into a fiber wherein said fiber has a weight average molecular weight of at least 700,000.
- IV. processing said fiber, optionally in combination with one or more other fibers, into a fabric;
- V. processing said fabric into said article;
- resulting in an article with improved alkali resistance.
A method of improving the warp direction stretch of a finished knit stretch fabric comprising the steps of:
- I. preparing an elastomer resin in an internal mixing device wherein said elastomer resin is prepared by reacting:
- (i) a hydroxyl terminated polyester intermediate derived from a dicarboxylic acid and a blend of at least two alkylene glycols wherein two of the alkylene glycols have a number average molecular weight that differs by at least 20 percent;
- (ii) a diisocyanate and
- (iii) a linear alkylene glycol chain extender;
- wherein the resulting resin has a weight average molecular weight of at least 600,000;
- and
- II. further reacting the resin composition with
- (iv) an agent comprising the reaction product of a polyalkylene ether glycol and a diisocyanate;
- and
- III. melt-spinning said elastomer resin into a fiber wherein said fiber has a weight average molecular weight of at least 700,000.
- IV. processing said fiber, optionally in combination with one or more other fibers, into a knit stretch fabric;
- resulting in a knit stretch fabric with improved warp direction stretch.
Dependencies are inferred from the claim text.