Process for producing poly (lactic acid) from lactic acid characterized by comprising the steps of:
- a) in an oligomerization reactor (R1), performing the polycondensation of a lactic acid solution by heat in the form of temperature ramps with a heating rate of 0.05° C. to 20° C. per minute until reaching a constant temperature in the range of 140° C.-170° C., keeping the reaction medium at this level for 30 minutes to 10 hours and with a controlled pressure in the range of 600 mmHg to 20 mmHg, obtaining low molar mass poly (lactic acid), oligomer, in the range of 300 to 5,000 g/mol;
- b) directing, via stream (L1), the low molar mass poly (lactic acid) obtained in step a) to an stirred storage tank (R10) and adding 1 to 5000 ppm of a depolymerization catalyst at a temperature between 120° C. and 180° C., obtaining a heated mixture;
- c) transferring the mixture obtained in step b), via stream (L2), to a depolymerization reactor (200) and effecting the depolymerization of the mixture obtained in step b) at a temperature between 190° C. and 240° C. in the presence of a depolymerization catalyst and at reduced pressure between 10 and 50 mmHg, obtaining a vapor stream (L3), which is directed to a first set of condenser and vessel (C2, R11) under reduced pressure between 10 and 100 mmHg and temperature between 160° C. and 240° C., in order to condense the components of a heavy fraction of the vapor stream (L3);
- d) directing, via stream (L4), the light and intermediate fractions of the vapor stream (L3) to a second set of condenser and vessel (C3, R2) at a temperature between 90° C. and 160° C., obtaining a lactide with purity between 70% and 90% (m/m), which is condensed into the vessel (R2), while the light fraction remains in the vapor phase;
- e) directing the light fraction to the condenser (C12) at temperatures between 10° C. and 50° C., obtaining a liquid light fraction that can be recycled through stream (RL3) to the reactor (RI);
- f) directing, via stream (L5), the lactide-rich stream from step d) to a stirred vessel (R3) for recrystallization of lactide in ethanol at a temperature between 60° C. and 100° C., cooling the solution after solubilization to 10° C. and allowing recrystallization for a period of 30 minutes to 12 hours;
- g) directing, via stream (L6), the recrystallized lactide obtained in step f) into a vessel (R4) for pre-polymerization of the recrystallized lactide via ring opening in the presence of a catalyst at a temperature between 90° C. and 200° C. for 10 to 60 minutes, for obtaining a low molar mass polylactide;
- h) pumping, via stream (L7), the polylactide obtained in step g) to a tubular reactor (300) for polymerization at a temperature between 160° C. and 220° C. for 1 to 3 hours, obtaining a polylactide with a molar mass between 50,000 and 200,000 g/mol and a reaction conversion between 70% and 95%;
- i) transferring, via stream (L8), the polylactide obtained in step h) to a devolatilizer (400) having a pear shaped structure (402), wherein at a temperature between 180° C. and 200° C. and under reduced pressure, residual lactide vapors are removed and sent to a condenser (C11), while devolatilized polylactide runs down the wall of the pear shaped structure (402) towards a horizontal extruder (500);
- and
- j) conforming the polylactide obtained in step i) in said extruder (500) and transferring the fluid polylactide into the final product granulation.