A sintered, generally spherical ceramic body, having an alumina content of from about 52 to about 58 weight percent distributed substantially homogeneously throughout the body, a silica content from about 32 to about 39 weight percent distributed substantially homogeneously throughout the body, an apparent specific gravity of about 2.63 to about 2.67, and a bulk density of about 1.48 to about 1.56 grams per cubic centimeter.
Claims18
A sintered, generally spherical ceramic body, comprising:
- an alumina content between about 32 and about 39 weight percent distributed substantially homogeneously throughout the body;
- a silica content between about 52 and about 58 weight percent distributed substantially homogeneously throughout the body;
- an apparent specific gravity of about 2.65;
- and
- a bulk density of about 1.50 grams per cubic centimeter.
A method of making a sintered, generally spherical ceramic pellet having an alumina content of between about 32 and about 35 weight percent, a silica content of between about 56 and about 59 weight percent, a specific gravity of about 2.65, a bulk density of about 1.44 grams per cubic centimeter, and less than about 10 percent crush at 7500 psi, comprising:
- pelletizing a raw material blend substantially comprising aluminosilicate and having an iron content of between about 1.5 and about 5.0 weight percent, a silica content of between about 56 and about 59 weight percent and an alumina content of between about 32 and about 35 weight percent;
- sintering the pellets at a temperature of between about 2345 and about 2420 degrees Fahrenheit for up to about 30 minutes.
A method of using sintered, generally spherical ceramic bodies having an alumina content of between about 32 and about 35 weight percent, a silica content of between about 56 and about 59 weight percent, a specific gravity of about 2.65, a bulk density of about 1.44 grams per cubic centimeter, and a crush of less than about 20 percent at 7000 psi to prop open a fracture in a subterranean geological formation, comprising in combination:
- injecting a pressurized fluid into a geological formation at a sufficient rate to fracture the same;
- injecting into the fracture a fluid containing sintered, generally spherical ceramic bodies into the fracture;
- and
- lodging a volume of sintered generally spherical ceramic bodies in the fracture;
- wherein the respective bodies are characterized by an alumina content of between about 35 and about 38 weight percent, a silica content of between about 54 and about 57 weight percent, a specific gravity of about 2.65, a bulk density of about 1.44 grams per cubic centimeter, and a crush of less than about 10 percent at 7500 psi.
A high strength propping agent for use in hydraulic fracturing of subterranean formations comprising a plurality of solid, substantially spherical particles, wherein the particles are characterized by an alumina content of between 35 and 38 weight percent, a specific gravity of between 2.61 and 2.65 grams per cubic centimeter and ambient temperature permeability of at least about 100,000 millidarcies at 8,000 psi.
Dependencies are inferred from the claim text.