Resin foam and foam sealing material
AssigneeNitto Denko Corporation
InventorsMakoto Saitou, Itsuhiro Hatanaka, Kazumichi Kato, Kiyoaki Kodama
Life of this patent
Estimating the term…
Loading patent…
AssigneeNitto Denko Corporation
InventorsMakoto Saitou, Itsuhiro Hatanaka, Kazumichi Kato, Kiyoaki Kodama
Estimating the term…
There is provided a resin foam excellent in dustproof performance, particularly dustproof performance in a dynamic environment. The resin foam of the present invention has a thickness recovery ratio of 65% or more, wherein the thickness recovery ratio is defined as a ratio of a thickness 1 second after releasing a compressed state to an initial thickness, when the resin foam is compressed for 1 minute in the thickness direction so as to give a thickness equal to 20% of the initial thickness in a 23° C. atmosphere; and then the compressed state is released in a 23° C. atmosphere.
A resin foam having a thickness recovery ratio of 65% or more, wherein the thickness recovery ratio is defined as a ratio of a thickness 1 second after releasing a compressed state to an initial thickness, when the resin foam is compressed for 1 minute in the thickness direction so as to give a thickness equal to 20% of the initial thickness in a 23° C. atmosphere;
Dependencies are inferred from the claim text.