Thermosetting epoxy-terminated oxazolidinone ring containing polymers which are obtainable by reacting at least one polyisocyanate compound with at least one hydroxy group containing epoxy resin and/or a combination of at least one epoxy resin and at least one di- or multifunctional nucleophilic compound that is capable of forming crosslinks between epoxy groups. The polymers have an onset glass transition temperature of at least about 45° C. and are capable of showing an onset glass transition temperature in the cured state at least about 160° C. Powder coating compositions comprising these polymers are also disclosed.
A thermosetting powder coating composition, wherein the composition comprises (a) a thermosetting polymer, wherein the polymer is obtainable by reacting at least one of (i) at least one hydroxy group containing epoxy resin and (ii) a combination of at least one epoxy resin and at least one di- or multifunctional nucleophilic compound that is capable of forming crosslinks between epoxy groups with (iii) at least one polyisocyanate compound in the presence of (iv) at least one catalyst which is capable of promoting a formation of oxazolidone rings and a branching of the polymer and wherein the polymer in an uncured state has an onset glass transition temperature of at least about 45° C. and is capable of showing an onset glass transition temperature in a cured state of at least about 160° C. and (b) one or more curing catalysts for (a).
A method of making an epoxy-terminated oxazolidinone ring containing polymer which has an onset glass transition temperature in an uncured state of at least about 45° C. and is capable of showing an onset glass transition temperature of up to about 160° C. in a cured state, wherein the method comprises (i) adding, under conditions which favor a formation of oxazolidinone rings over a formation of isocyanurate rings, at least one polyisocyanate compound to a mixture of (al) at least one hydroxy group containing epoxy resin and/or (a2) a combination of at least one epoxy resin and at least one di- or multifunctional nucleophilic compound that is capable of forming crosslinks between epoxy groups and (b) at least one compound which is capable of catalyzing a reaction between epoxy groups and isocyanate groups and is capable of promoting a branching of the polymer;