Method of manufacture of homodispersed silicon carbide-derived carbon composites
AssigneeOû Skeleton Technologies
InventorsJaan Leis, Mati Arulepp
Life of this patent
Estimating the term…
Loading patent…
AssigneeOû Skeleton Technologies
InventorsJaan Leis, Mati Arulepp
Estimating the term…
The present invention concerns a method of manufacture of the homodispersed composite of the synthetic carbon material derived from carbide and silicon where the powder of the carbon material is first dispersed mechanically with the powder of silicon to homodispersed mixture, then the homodispersed mixture of the carbon material and silicon is sintered in an inert environment at a temperature between 1200 to 1500° C. to synthetic homodispersed composite of the silicon carbide and silicon. The homodispersed composite of the silicon carbide and silicon is heated in an inert environment at a temperature between 800 to 1100° C. and then the homodispersed composite of the silicon carbide and silicon is chlorinated at a temperature from 800 to 100° C.
1-17. (canceled)
A method for preparing a homodispersed composite of carbide derived synthetic carbon material and silicon that comprises stages in where:
Dependencies are inferred from the claim text.