Method of Manufacture of Article for Delivering Health-Benefit Agent
AssigneeKimberly-Clark Worldwide, Inc.
InventorsPeiguang Zhou, David Gerard Iwanski, Gary Alan Turchan, Stephen David Franger
Life of this patent
Estimating the term…
Abstract
A laminate of nonwoven materials having fine particulate matter attached thereto is made with a lamination process capable of supplying up to about 60 gsm of particulate matter to a substrate. The particulate matter may be applied to the substrate using a powder coating apparatus. The laminate may be used in personal absorbent articles such as diapers, feminine pads, bandages, bed pads, and the like.
Claims20
A method for constructing a laminate comprising the steps of:
- fluidizing an amount of particulate matter, wherein the particulate matter is selected from a group consisting of menthol, activated charcoal, carbon, silica gel, xylitol, clay, dessicants, prebiotics, probiotics, surfactants, anti-oxidants, disinfectants, antibacterial agents, antiviral agents, pharmaceutical actives, perfumes, deodorants, opacifiers, astringents, preservatives, superabsorbent material and a combination thereof;
- creating a base by
- conveying at a speed of 30 to 600 meters/minute a first substrate and a second substrate, each having an inner surface and an outer surface;
- attaching a first adhesive layer to the inner surface of the first substrate;
- and
- applying an amount of the fluidized particulate matter onto the first adhesive layer to create a first layer of particulate matter;
- creating a cover by attaching a second adhesive layer to the inner surface of the second substrate;
- and
- attaching the base to the cover so that the outer surfaces of the first substrate and the second substrate are exposed.
A method for constructing a nonwoven laminate comprising the steps of:
- (1) fluidizing an amount of particulate matter;
- (2) conveying a first nonwoven substrate and a second nonwoven substrate;
- (3) attaching a first adhesive layer to an inner surface of the first nonwoven substrate;
- (4) electrostatically attaching a first layer of particulate matter to the first adhesive layer at a basis weight of 8 gsm to 40 gsm, the particulate matter having a particle size of 2 microns to 120 microns;
- (5) attaching a second adhesive layer to an inner surface of the second nonwoven substrate;
- and
- (6) attaching the second adhesive layer to the first layer of particulate matter.
The method of 17 further comprising the step of reclaiming excess particulate matter.
Dependencies are inferred from the claim text.