Methods for Producing a Coated Abrasive Article for Polishing or Lapping Applications
OwnerOlivier L. Guiselininventor
Life of this patent
Estimating the term…
Abstract
Methods are provided for forming an abrasive coating on a surface of a backing. An abrasive slurry includes a continuous phase, a first discontinuous phase of abrasive particles dispersed in the continuous liquid phase, and a second discontinuous phase of binder precursor particles dispersed in the continuous liquid phase, so that the continuous liquid phase carries the first and second discontinuous phases. A coated abrasive article is formed by coating the abrasive slurry onto the surface of the backing, and then removing the continuous phase.
Claims20
A method of manufacturing a coated abrasive article comprising:
- (a) providing a flexible backing having a surface configured for being coated with an abrasive coating;
- (b) providing an abrasive slurry including a continuous liquid phase, which comprises at least 50% per weight of water, and at least 0.001% per weight of fluorosurfactant;
- a first discontinuous phase including abrasive particles dispersed in the continuous liquid phase;
- and
- a second discontinuous phase including a waterborne binder precursor particle dispersion in the continuous liquid phase,
- wherein the continuous liquid phase carries the first and second discontinuous phases,
- wherein the volume ratio of abrasive particles to binder precursor particles is 0.05 to 3, and wherein the first and the second discontinuous phases comprise between 5% and 60% of the abrasive slurry by volume;
- (c) coating the abrasive slurry onto the surface of the flexible backing;
- (d) removing at least 50% per weight of the continuous liquid phase by evaporation;
- and
- (e) coalescing the binder precursor particles at the surface of the flexible backing to form a coating with solid continuous binder phase disposed about the abrasive particles.
A method of manufacturing a coated abrasive article comprising:
- (a) providing a flexible backing having a surface configured for being coated with an abrasive coating;
- (b) providing an abrasive slurry including
- a continuous liquid phase, which comprises at least 60% per weight of water, and at least 0.001% per weight of fluorosurfactant;
- a first discontinuous phase including abrasive particles dispersed in the continuous liquid phase;
- and
- a second discontinuous phase including a waterborne binder precursor particle dispersion in the continuous liquid phase,
- wherein the continuous liquid phase carries the first and second discontinuous phases, wherein the volume ratio of abrasive particles to binder precursor particles is 0.05 to 3, wherein the first and the second discontinuous phases comprise between 5% and 60% of the abrasive slurry by volume, and wherein the viscosity of the abrasive slurry is less than 100,000 cP;
- (c) coating the abrasive slurry onto the surface of the flexible backing;
- (d) removing at least 60% per weight of the continuous liquid phase by evaporation;
- and
- (e) coalescing the binder precursor particles at the surface of the flexible backing.
A method of manufacturing a coated abrasive article comprising:
- (a) providing a flexible backing having a surface configured for being coated with an abrasive coating,
- wherein the flexible backing is selected from the group consisting of plastic film, metallic foil, cloth, paper, foam and combinations thereof;
- (b) providing an abrasive slurry including a continuous liquid phase, which comprises at least 90% per weight of water, and at least 0.01% per weight of fluorosurfactant;
- a first discontinuous phase including abrasive particles dispersed in the continuous liquid phase;
- and
- a second discontinuous phase including a waterborne binder precursor particle dispersion in the continuous liquid phase,
- wherein the continuous liquid phase carries the first and second discontinuous phases, wherein the volume ratio of abrasive particles to binder precursor particles is 0.05 to 2, and wherein the first and the second discontinuous phases comprise between 10% and 40% of the abrasive slurry by volume;
- wherein the waterborne binder precursor particle dispersion is selected from the group consisting of waterborne acrylics emulsion, waterborne polyurethanes dispersion, waterborne urethane-acrylic copolymers dispersion, waterborne polyesters dispersion, waterborne alkyds dispersion, waterborne epoxies dispersion, waterborne phenoxy dispersion, waterborne melamine dispersion, waterborne polyamide dispersion, waterborne polyimide dispersion, waterborne cyanate esters dispersion, and combinations thereof;
- wherein the continuous liquid phase comprises a curing agent selected from the group consisting of metal ion crosslinkers, polyaldehydes, polyaziridines, polyisocyanates, polysulfides, imidazoles, dicyandiamines, polyamidoamines, polyamides, polyamines, functionalized silanes, functionalized siloxane, carbodiimides, peroxides, and combinations thereof.
- (c) coating the abrasive slurry onto the surface of the flexible backing;
- (d) removing at least 90% per weight of the continuous liquid phase by evaporation;
- (e) coalescing the binder precursor particles at the surface of the flexible backing to form a coating with solid continuous binder phase disposed about the abrasive particles;
- and
- (f) thermally curing the coating using at least one energy source.
Dependencies are inferred from the claim text.