Shear-Stable High Viscosity Polyalphaolefins
AssigneeExxonMobil Chemical Company - Law Technology
InventorsMargaret May-Som Wu, Kevin B. Stavens, Wenning W. Han, Abhimanyu O. Patil
Life of this patent
Estimating the term…
Loading patent…
AssigneeExxonMobil Chemical Company - Law Technology
InventorsMargaret May-Som Wu, Kevin B. Stavens, Wenning W. Han, Abhimanyu O. Patil
Estimating the term…
A polyalphaolefin polymer, having a kinematic viscosity at 100° C. of 135 cSt or greater, is shear stable. The polymer either has not more than 0.5 wt % of the polymer having a molecular weight of greater than 60,000 Daltons, or after being subjected to twenty hours of taper roller bearing testing, the polymer has a kinematic viscosity loss of less than 9%. Such a shear stable polyalphaolefin is obtained by either mechanical breakdown of a high viscosity polyalphaolefin or by a selective catalyst system used in oligomerization or polymerization of the feedstock.
A polyalphaolefin polymer, wherein the polyalphaolefin polymer has a kinematic viscosity at 100° C. of 135 cSt or greater and is derived from not more than 10 mol % ethylene, wherein the polyalphaolefin polymer is characterized by, after being subjected to twenty hours of a taper roller bearing testing, having a kinematic viscosity loss of less than 9%.
A polyalphaolefin polymer, wherein the polyalphaolefin polymer has a kinematic viscosity at 100° C. of 135 cSt or greater and is derived from not more than 10 mol % ethylene, wherein the polyalphaolefin polymer is characterized by not more than 0.5 wt % of the polymer having an molecular weight of greater than 60,000 Daltons.
A polyalphaolefin polymer, wherein the polyalphaolefin polymer has a kinematic viscosity at 100° C. of 135 cSt or greater, wherein the polyalphaolefin polymer is characterized by, after being subjected to twenty hours of taper roller bearing testing, an oxygen content of not more than 0.5 oxygen molecules per 100 carbon molecules.
Dependencies are inferred from the claim text.