Equipment for use in corrosive environments and methods for forming thereof
AssigneeChevron U.S.A. Inc.
InventorsEdwin Hall Niccolls, Grzegorz Jan Kusinski, David Lawrence Cooke
Life of this patent
Estimating the term…
Loading patent…
AssigneeChevron U.S.A. Inc.
InventorsEdwin Hall Niccolls, Grzegorz Jan Kusinski, David Lawrence Cooke
Estimating the term…
A method for forming structural equipment employed in sulfur containing environments such as oil refineries and the like. In one embodiment, the method comprises: providing a steel composition containing up to 0.35% of C, 0.30 to 3.5% Si, up to 1.2% Mo, up to 1.35% Mn, up to 5% Al, less than 12.0% Cr, balance of Fe and unavoidable impurities; forming a structural component conforming to prevailing industry standards with respect to design, fabrication, inspection and testing, metallurgical and mechanical properties. The structural equipment has a corrosion rate of less than 15 mpy. In one embodiment, the equipment is formed from a steel composition has a carbon equivalent of less than 0.63, requiring no post weld heat treatment (“PWHT”). In another embodiment, the CE is less than 0.45, requiring no preheat nor PWHT.
A method for forming a corrosion resistant structural equipment, the method comprising:
Dependencies are inferred from the claim text.