Boron-Containing Nucleating Agent for Polyphenylene Sulfide
AssigneeTicona LLC
InventorKe Feng
Life of this patent
Estimating the term…
Loading patent…
AssigneeTicona LLC
InventorKe Feng
Estimating the term…
A boron-containing nucleating agent is provided for use with a polyarylene sulfide. The boron-containing nucleating agent can have low crystallinity, a small particle size, and a large specific surface area. By selectively controlling certain aspects of the nucleating agent, the crystallization properties of a thermoplastic composition including the nucleating agent and a polyarylene sulfide can be significantly improved. For instance, the recrystallization temperature can be increased, which can allow the “cooling time” during a molding cycle to be substantially reduced. Through use of the boron-containing nucleating agent the recrystallization temperature can be greater than about 231° C.
A thermoplastic composition comprising a boron-containing nucleating agent and a polyarylene sulfide, the boron-containing nucleating agent having a graphitization index of greater than about 4, the nucleating agent having an average particle size and a specific surface area, wherein the ratio of the average particle size to the specific surface area is between about 0.001 and about 1 micrometers per square meter per gram, the thermoplastic composition having a recrystallization temperature of greater than about 231° C. as determined according to differential scanning calorimetry.
A method for molding a thermoplastic composition, the method comprising:
Dependencies are inferred from the claim text.