Sheet width control for overflow downdraw sheet glass forming apparatus
AssigneeCorning Incorporated
InventorRichard B. Pitbladdo
Life of this patent
Estimating the term…
Abstract
A method keeps the width of the manufactured sheet substantially the same by attaching edge directors for the formed sheet to the manufacturing apparatus structure instead of to the forming block. Thus, sheet glass may be manufactured to specification for a longer time with the same forming block. An additional method adjusts the width of the manufactured sheet by changing the distance between the edge directors. Thus sheet glass may be manufactured to different width specifications with the same forming block.
Claims61
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by at least one edge director on each end of the forming block, wherein the improvement comprises:
- a) a far end edge director fixed to a far end of the forming block;
- and
- b) an inflow end edge director fixed to a support structure at an inflow end of the forming block;
- such that a surface of the forming block at the inflow end can move relative to the inflow end edge director as the forming block changes shape due to thermal creep without changing a distance between the far end edge director and the inflow end edge director, such that a width of a glass sheet remains constant.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- a) a far end edge director fixed to a support structure at a far end of the forming block;
- b) an inflow end edge director fixed to a support structure at an inflow end of the forming block;
- and
- c) a first adjustment device that adjusts a position of the forming block relative to the far end edge director and the inflow end edge director;
- such that a surface of the forming block can be moved relative to both the inflow end edge director and the far end edge director as the forming block changes shape due to thermal creep without changing a distance between the far end edge director and the inflow end edge director, such that a width of a glass sheet remains constant.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- a) an inflow end edge director fixed to an inflow end of the forming block;
- and
- b) a far end edge director fixed to a support structure at a far end of the forming block;
- such that a surface of the forming block at the far end can move relative to the far end edge director as the forming block changes shape due to thermal creep without changing a distance between the inflow end edge director and the far end edge director, such that a width of a glass sheet remains constant.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- a) a far end edge director fixed to a far end of the forming block;
- and
- b) an inflow end support assembly comprising an inflow pipe, a support block surface, and an inflow end edge director fixed to a stationary apparatus support structure at an inflow end of the forming block;
- such that a surface of the forming block at the inflow end can move relative to the inflow end edge director as the forming block changes shape due to thermal creep without changing a distance between the far end edge director and the inflow end edge director, such that a width of a glass sheet remains constant.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- a) a far end support assembly comprising a support block surface and a far end edge director fixed to a stationary apparatus support structure at a far end of the forming block;
- b) an inflow end support assembly comprising an inflow pipe, a support block surface, and an inflow end edge director fixed to the stationary apparatus support structure at an inflow end of the forming block;
- and
- c) an adjustment device that can adjust a position of the forming block relative to the far end edge director and the inflow end edge director;
- such that a surface of the forming block can be moved relative to both the inflow end edge director and the far end edge director as the forming block changes shape due to thermal creep without changing a distance between the inflow end edge director and the far end edge director, such that a width of a glass sheet remains constant.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- an inflow end support assembly comprising an inflow pipe, a support block surface, and at least one inflow end edge director, wherein a location of the inflow end edge director is fixed relative to the inflow pipe and the support block surface for the forming block.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- an inflow end compression block that is mounted at an angle to partially support a weight of the forming block such that a friction force counteracting a compression force is reduced.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- a) an inflow end support assembly that surrounds an inflow end of the forming block and allows glass to completely envelop the inflow end of the forming block;
- and
- b) a far end support assembly that surrounds a far end of the forming block and allows glass to completely envelop the far end of the forming block;
- wherein the forming block is completely enveloped with glass during production operation to protect the forming block from oxidation;
- and
- wherein the forming block is made from molybdenum.
An improved apparatus for forming sheet glass, wherein the apparatus includes an inflow pipe for delivering molten glass, a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming block and meets at the bottom of the wedge, the width of the glass flowing down the sloping sides being defined by edge directors on each end of the forming block, wherein the improvement comprises:
- at least one glass seal, wherein the glass seal facilitates an application of force from at least one force motor external to the apparatus to the forming block.
A method for manufacturing glass sheets using an apparatus that includes a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the a wedged shaped sheet foaming block and meets at the bottom of wedge, wherein the method comprises the step of:
- moving a surface of the forming block relative to at least one end edge director fixed to support structure at that end of the forming block as the forming block changes shape due to thermal creep without changing a distance between a far end edge director at a far end of the forming block and an inflow end edge director at an inflow end of the forming block, such that a width of a glass sheet remains constant.
A method for manufacturing glass sheets using an apparatus that includes a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the a wedged shaped sheet forming block and meets at the bottom of wedge, wherein the method comprises the step of:
- adjusting a longitudinal position of the forming block relative to an inflow end edge director and a far end edge director to maintain a formed sheet glass thickness profile.
(canceled)
A method for manufacturing glass sheets using an apparatus that includes a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the wedged shaped sheet forming structure and meets at the bottom of wedge, wherein the method comprises the step of:
- adjusting a mass flow of glass times a viscosity of glass as the forming block changes shape due to thermal creep without changing a distance between a far end edge director and. an inflow end edge director, such that a width of a glass sheet and a thickness of the glass sheet remain constant.
A method for manufacturing glass sheets using an apparatus that includes a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the a wedged shaped sheet forming block and meets at the bottom of wedge, wherein the method comprises the step of:
- adjusting an angle of the forming block to horizontal as the forming block changes shape due to thermal creep without changing a distance between a far end edge director and an inflow end edge director, such that a width of a glass sheet and a thickness of the glass sheet remain constant.
(canceled)
A method for manufacturing glass sheets using an apparatus that includes a trough for receiving molten glass that has sides attached to a wedged shaped sheet forming block that has downwardly sloping sides converging at the bottom of the wedge such that a glass sheet is formed when molten glass flows over the sides of the trough, down the downwardly sloping sides of the a wedged shaped sheet forming block and meets at the bottom of wedge, wherein the method comprises the steps of:
- a) changing a sheet width by changing a distance between a far end edge director and an inflow end edge director;
- and
- b) adjusting an angle of the forming block to horizontal when changing the sheet width, such that thickness of the sheet remains constant.
55-65. (canceled)
(canceled)
71-72. (canceled)