Abstract
An optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.
Claims20
An optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.
An image display device having an optical film on the display surface of the panel thereof, wherein the optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.
A polarizer having a polarizing element and an optical film, wherein the optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.
A liquid-crystal display device at least having a polarizer having a polarizing element and an optical film, wherein the optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.
Dependencies are inferred from the claim text.