Abstract
A method for restoring a silver oxide-containing hydrophilic coating includes heating the coating to a temperature between about 260° C. and about 540° C. and maintaining the coating at a temperature between about 260° C. and about 540° C. in an environment containing oxygen and ozone for less than 24 hours.
Claims20
A method for restoring a silver oxide-containing hydrophilic coating, the method comprising:
- heating the coating to a temperature between about 260° C. and about 540° C.;
- and
- maintaining the coating at a temperature between about 260° C. and about 540° C. in an environment containing oxygen and ozone for less than 24 hours.
A method for preparing a component having a silver oxide-containing hydrophilic coating, the method comprising:
- heating the component to a first temperature between about 370° C. and about 540° C.;
- maintaining the component at the first temperature for between about 1 hour and about 4 hours in an environment containing oxygen and ozone to eliminate contaminants from the coating;
- reducing the temperature of the component to a second temperature between about 260° C. and about 510° C.;
- and
- maintaining the component at the second temperature for between about 15 minutes and about 4 hours in the environment containing oxygen and ozone.
A method for restoring a condensing heat exchanger having an antimicrobial hydrophilic coating, the method comprising:
- heating the heat exchanger to a first temperature between about 370° C. and about 540° C.;
- maintaining the heat exchanger at the first temperature for less than about 24 hours in an environment containing oxygen and ozone to eliminate contaminants from the coating;
- reducing the temperature of the heat exchanger to a second temperature between about 260° C. and about 510° C.;
- and
- maintaining the heat exchanger at the second temperature for between about 15 minutes and about 4 hours in the environment containing oxygen and ozone to reform silver oxide.