Wound Healing Device, Method for Making the Same and Method for Treating a Wound
OwnerMohammad Rezaul Karim, Abdulrahman M. Al-Ahmari +3inventors
InventorsMohammad Rezaul Karim, Abdulrahman M. Al-Ahmari, Saeed M. Al-Zahrani, Jeong Hyun Yeum, Kil-Soo Kim
Life of this patent
Estimating the term…
Abstract
A wound healing device includes a mat of aligned nanofibers of polyaniline, o-aminobenzenesulfonic acid copolymer, polyvinyl alcohol and chitsosan oligossacaride. Method for fabricating the mat and treating wounds are also disclosed.
Claims9
A wound healing device for promoting enhanced healing of a wound comprises:
- a mat of aligned conductive nanofibers polyaniline and o-aminobenzenesulfonic acid copolymer, vinyl alcohol and chitosan oligossacaride.
A method for preparing a nanofiber wound healing device comprising the steps of
- providing a mass of aniline, o-aminobenzenesulfonic acid PVA and chitosan oligossacaride (COS);
- chemically perimerizing the aniline and o-aminobenzenesulfonic acid using ammonium persulfate as an oxidant and maintaining the oxicant/monomer ratio at 1 to form a PAni-co-PABSA copolymer;
- preparing a PVA solution in double distilled water at 80° C. under magnetic stirring for 2 hours;
- cooling the PVA solution to room temperature;
- dissolving chitosan oligossacaride powder in double distilled water under magnetic stirring for 1 hour at room temperature and adding the PVA solution and the PAni-co-PABSA copolymer to form PAni-co-PABSA/PVA/COS blend solution;
- and
- electro spinning the PAni-co-PABSA/PVA/COS blend solution at high voltage power and collect fibers on an electrically grounded aluminum foil to form a nanofiber mat.
A method for preparing a wound healing and wound size reduction consisting of the following steps:
- preparing a copolymer of aniline, o-aminobenzenesulfonic acid and chemically polymerizing in aniline and o-aminobenzenesulfonic acid in an aqueous solution of 1.2M HCl using ammonium persulfate as an oxidant;
- maintaining the oxidant/monomer ration of 1;
- dissolving the aniline and o-aminobenzenesulfonic acid in 200 ml of 1.2 M HCL solution to produce a monomer solution;
- dissolving 4.56 g of ammonium persulfate in 100 ml of 1.2 M HCL and then adding slowly to the monomer solution with constant stirring at room temperature for 24 hours to form a copolymer powder;
- filtering out the copolymer powder and washing with a small amount of 1.2 M HCL until the filtered solution is colorless to thereby obtain a green powder;
- drying the green powder under a vacuum for 48 hours;
- preparing a 7.5 wgt. % PVA solution in double distilled water at 80° C. with magnetic stirring for 2 hours and cooling to room temperature;
- dissolving 12.5 wgt. % of COS powder in double distilled water with magnetic stirring for 1 hours at room temperature;
- preparing a PAni-co-PABSA/PVA/Cos blend solution by mixing bulk PAni-co-PABSA (3 wgt. %), PVA (7.5 wgt. %) and COS (12.5 wgt. %) with the content of between 1:8:1 to 1:16:3 in aqueous solution at room temperature with gentle stirring for 2 hours;
- and
- electrospinning the PAni-co-PABSA/PVA/COS solution at 5-20 KV from a blunt needle tip via a syringe pump to control the solution flow rate and collecting fibers on an electrically grounded aluminum foil placed at 5-20 cm vertical distance from the needle tip.
A method for treating a wound by applying an aligned nanofiber mat of PAni-co-PABSA/PVA/COS nanofiber to the wound for a period of 15 days.
Dependencies are inferred from the claim text.