US 2012/0231093 A1Published application
Method for preparing nano-scale or amorphous particle using solid fat as a solvent
OwnerKab-Sig KIMinventor
Life of this patent
Estimating the term…
Abstract
The present invention relates to a method for preparing nanoscale or amorphous particles using solid fat as a solvent. According to the present invention, nanoscale or amorphous particles of active ingredients are prepared by using fat as a solvent, wherein the fat is in solid phase at room temperature. The nanoscale or amorphous particles of active ingredients can be advantageously used in medicine, cosmetics, functional foods or the like.
Claims26
-2. (canceled)
A method for preparing nanoscale particles comprising the steps of:
- (1) preparing a mixture comprising one or more active ingredients and solid fat as a solvent in an excess amount to the active ingredient, and
- (2) pressurizing the mixture comprising one or more active ingredients and solid fat to the critical pressure or more by adding the gas of a supercritical fluid into the mixture, then removing the solid fat from the mixture by releasing out the solid fat together with the gas of the supercritical fluid, wherein the supercritical fluid is CO2 or N2 and wherein the temperature is maintained below the melting point of the solid fat;
- and,
- wherein the step (1) further comprises rapidly cooling the homogeneously melt-mixed mixture for solidification;
- pulverizing the solidified mixture;
- adding one or more surfactants and/or one or more non-surfactant type anti-coagulating agents or aqueous solution thereof to the pulverized powder and mixing them homogeneously;
- and drying the mixed product at room temperature.
4 more elements
A method for preparing nanoscale particles comprising the steps of:
- (1) preparing a mixture comprising one or more active ingredients and solid fat as a solvent in an excess amount to the active ingredient, and
- (2) pressurizing the mixture comprising one or more active ingredients and solid fat to the critical pressure or more by adding the gas of a supercritical fluid into the mixture, and then removing the solid fat from the mixture by releasing out the solid fat together with the gas of the supercritical fluid, wherein the supercritical fluid is CO2 or N2 and wherein the temperature is maintained below the melting point of the solid fat,
- wherein the step (1) comprises:
- adding one or more surfactants and solid fat into a reactor, and melt-mixing them homogenously;
- rapidly cooling the homogenously melt-mixed mixture for solidification;
- pulverizing the solidified mixture;
- adding one or more surfactants and/or one or more non-surfactant type anti-coagulating agents together with one or more active ingredients or aqueous solution thereof, to the pulverized powder and mixing them homogenously;
- and drying the mixed product at room temperature.
5 more elements
-7. (canceled)
Dependencies are inferred from the claim text.