Method for forming a tubular medical device
AssigneeICON Medical Corp.
InventorsRaymond W. Buckman, JR., Udayan Patel, Joseph Furst
Life of this patent
Estimating the term…
Abstract
A method and process for at least partially forming a medical device that is at least partially formed of a metal alloy which improves the physical properties of the medical device.
Claims19
1-26. (canceled)
A method for forming a medical device comprising the steps of:
- a) forming a rod or tube having a surface and an outer cross-sectional area, said rod or tube including a metal alloy that is formed of at least about 95 weight percent of a solid solution of molybdenum and rhenium or tungsten and tantalum;
- b) drawing down said outer cross-sectional area of said rod or tube by a reducing mechanism;
- c) annealing said rod or tube at an annealing temperature in an oxygen reducing environment or inert environment after said rod or tube has been drawn down;
- d) cooling said annealed rod or tube at a rate of at least about 100° C. per minute;
- e) drawing down said cross-sectional area of said rod or tube by the reducing mechanism after said rod or tube has been annealed;
- and,
- f) annealing said rod or tube at least one additional time at an annealing temperature that is lower temperature than at least one annealing temperature of a previous annealing of said rod or tube.
The method as defined in claim 1, wherein said metal alloy includes about 41-49 weight percent rhenium, about 51-59 weight percent molybdenum, and up to about 1 weight percent additional metal, said additional metal including a metal selected from the group consisting of titanium, yttrium, zirconium, or mixtures thereof
A method for forming a stent comprising the steps of:
- a) forming a tube having a surface and an outer cross-sectional area, said tube formed of a metal alloy comprising about 41-49 weight percent rhenium, about 51-59 weight percent molybdenum;
- b) drawing down said outer cross-sectional area of said tube by a reducing mechanism;
- c) nitriding said tube to form a nitride layer on said tube prior to at least one of said drawing down steps, said step of nitriding including i) exposing at least a portion of said tube to a nitriding gas that includes nitrogen, nitrogen and hydrogen, or combinations thereof, and b) exposing at least a portion of said tube to a nitriding gas at a temperature of less than about 400° C. for at least about 1 minute, said nitride layer removed prior to said tube being annealed;
- d) annealing said tube at an annealing temperature in an oxygen reducing environment or inert environment after said tube has been drawn down;
- e) cooling said annealed tube at a rate of at least about 100° C. per minute;
- f) drawing down said cross-sectional area of said tube by the reducing mechanism after said rod or tube has been annealed, said step of drawing down said cross-sectional area of said tube reduces said cross-sectional area by less than about 20% each time said tube is processed by said reducing mechanism;
- g) annealing said rod or tube at least one additional time at an annealing temperature that is lower temperature than at least one annealing temperature of a previous annealing of said rod or tube, said steps of annealing said tube include the steps of a) annealing said tube at an annealing temperature of at least about 1480° C. for a time period of at least about 5 minutes for a time period of at least about 5 minutes when said tube has wall thickness of greater than about 0.015 inch, b) annealing said tube at an annealing temperature of about 1450-1480° C. for a time period of at least about 5 minutes when said tube has wall thickness of about 0.008-0.015 inch, and c) annealing said tube at an annealing temperature of less than about 1450° C. for a time period of at least about 5 minutes when said tube has wall thickness of less than about 0.008 inch;
- h) protecting said tube from oxygen when said tube is exposed to temperatures of greater than about 400-500° C.;
- and,
- i) cutting said tube to form said stent, said stent formed of a cut tube having an average grain size of 4-14 ASTM.
Dependencies are inferred from the claim text.