Oxygen Tailoring of Polyethylene Resins
AssigneeUnivation Technologies, LLC
InventorsSandra D. Schregenberger, James F. Lottes, Pradeep P. Shirodkar, Porter C. Shannon
Life of this patent
Estimating the term…
Loading patent…
AssigneeUnivation Technologies, LLC
InventorsSandra D. Schregenberger, James F. Lottes, Pradeep P. Shirodkar, Porter C. Shannon
Estimating the term…
A process is provided for extruding a bimodal polyethylene resin. The process includes providing a polyethylene homopolymer or copolymer resin having a bimodal molecular weight distribution; conveying the resin through an extruder having a feed zone in which the resin is not melted, a melt-mixing zone in which at least a portion of the resin is melted, and a melt zone in which the resin is in a molten state, each zone being partially filled with the resin; and contacting the molten resin in the melt zone with a gas mixture of 8 to 40% by volume O2. The resin can be further pelletized. The oxygen-tailored resin can be used to make polyethylene films having improved bubble stability.
1-19. (canceled)
A process for extruding a bimodal polyethylene resin, the process comprising:
The process of claim 1, wherein the bimodal polyethylene resin is a copolymer of ethylene and at least one comonomer selected from the group consisting of C3 to C12 alpha-olefins.
The process of claim 1, wherein the bimodal polyethylene resin has a density of at least 0.93 g/cm3.
The process of claim 1, wherein the bimodal polyethylene resin has a density of at least 0.945 g/cm3.
The process of claim 1, wherein the bimodal polyethylene resin has a density of from 0.93 to 0.97 g/cm3.
The process of claim 1, wherein the gas mixture comprises 10 to 35% by volume O2.
The process of claim 1, wherein the gas mixture comprises 15 to 25% by volume O2.
The process of claim 8, wherein the supported bimetallic catalyst comprises a non-metallocene transition metal catalyst and a metallocene transition metal catalyst.
The process of claim 8, wherein the monomers comprise ethylene and at least one C3-C12 alpha olefin.
The process of claim 1, further comprising after step (c) pelletizing the oxygen-treated resin.
The process of claim 1, wherein the bimodal polyethylene resin comprises a low molecular weight component and a high molecular weight component where the relative weight fraction of the high molecular weight component to the low molecular weight component is in the range of from 1:9 to 9:1.
Dependencies are inferred from the claim text.