Thermoplastic polymer mixtures, and applications thereof
AssigneeSolvay Advanced Polymers, L.L.C.
InventorsMohammad Jamal El-Hibri, Edward Ryan, Brian A. Stern
Life of this patent
Estimating the term…
Loading patent…
AssigneeSolvay Advanced Polymers, L.L.C.
InventorsMohammad Jamal El-Hibri, Edward Ryan, Brian A. Stern
Estimating the term…
Thermoplastic polymer mixture (M) comprising at least one poly(aryl ether ketone) (P1), at least one poly(arylene sulfide) (P2), and between 0 and 25 wt. % of the total weight of the thermoplastic mixture (M), of a thermoplastic polymer material (P3) consisting of (i) at least one poly(biphenyl ether sulfone) (P3a), and/or (ii) at least one poly(ether imide) (P3b), and/or at least one poly(ether imide sulfone) (P3c), wherein: the combined weight amount of the poly(aryl ether ketone) (P1) and the poly(arylene sulfide) (P2), based on the total weight of the polymer mixture (M), is of at least 30%, and the weight amount of the poly(aryl ether ketone) (P1), based on the combined weight of the poly(aryl ether ketone) (P1) and the poly(arylene sulfide) (P2), is of at most 90%.
A thermoplastic polymer mixture (M) comprising
The mixture according to any one of the preceding claims, wherein the weight amount of the poly(aryl ether ketone) (P1), based on the combined weight of the poly(aryl ether ketone) (P1) and the poly(arylene sulfide) (P2), is of at least 50%.
The mixture according to any one of the preceding claims, wherein the poly(aryl ether ketone) (P1) is a poly(ether ether ketone), preferably a poly(ether ether ketone) homopolymer.
The mixture according to any one of the preceding claims, wherein the poly(arylene sulfide) (P2) is a poly(phenylene sulfide), preferably a poly(phenylene sulfide) homopolymer.
The mixture according to any one of the preceding claims, wherein the thermoplastic polymer material (P3) consists of at least one polyphenylsulfone, preferably a polyphenylsulfone homopolymer.
The mixture according to any one of the preceding claims, which further comprises one or more additives selected from the group consisting of thermal stabilizers, processing aids, flame retardants, colorants, nucleating agents, impact modifiers, and mixtures thereof.
The mixture according to any one of the preceding claims, which further comprises at least one friction reducing additive.
Use of a thermoplastic polymer material (P3) consisting of (i) at least one poly(biphenyl ether sulfone) (P3a), and/or (ii) at least one poly(ether imide) (P3b), and/or at least one poly(ether imide sulfone) (P3c), for increasing the notched Izod and/or the tensile yield elongation and/or the tensile elongation at break and/or the heat deflection temperature of a thermoplastic polymer mixture comprising at least one poly(aryl ether ketone) (P1) and at least one poly(arylene sulfide) (P2).
Dependencies are inferred from the claim text.