Abstract
A method and apparatus produces high strength aluminum alloys from a powder containing L12 intermetallic dispersoids. The powder is degassed, sealed under vacuum in a container, heated, consolidated by vacuum hot pressing, and extruded.
Claims22
A method for producing a high strength aluminum alloy billet containing L12 dispersoids, comprising the steps of:
- placing a quantity of an aluminum alloy powder containing an L12 dispersoid therein having a mesh size of less than 450 mesh in a container;
- vacuum degassing the powder at a temperature of about 300° F. (149° C.) to about 900° F. (482° C.) for about 0.5 hours to about 8 days;
- sealing the degassed powder in the container under vacuum;
- heating the sealed container at about 300° F. (149° C.) to about 900° F. (482° C.) for about 15 minutes to eight hours;
- vacuum hot pressing the heated container to form a billet;
- and
- removing the container from the formed billet.
4 more elements
Apparatus for producing a high strength aluminum alloy billet containing L12 dispersoids, comprising:
- a container for holding a quantity of an aluminum alloy powder containing an L12 dispersoid therein having a mesh size of less than 450 mesh;
- a vacuum and heat source for degassing the powder at a temperature of about 300° F. (149° C.) to about 900° F. (482° C.) for about 0.5 hours to about 8 days;
- sealing means for sealing the degassed powder in the container under vacuum;
- a heater for heating the sealed container at about 300° F. (149° C.) to about 900° F. (482° C.) for about 15 minutes to eight hours;
- a vacuum hot press for forming the heated container into a billet;
- and
- means for removing the container from the thus formed billet.
4 more elements