Process for separating and refining impurities from lead bullion
OwnerMiguel Pizzuto, Robert Seebeck +1inventors
InventorsMiguel Pizzuto, Robert Seebeck, Jerry D. Schulz
Life of this patent
Estimating the term…
Abstract
The Razor Process™ is a unique pyrometallurgical lead refining process. Benefits from the Razor process™ include: lower energy costs; improved working environment; reduced recycling costs; increased refining productivity; reduced cycle time and labor requirements; and production of secondary recyclable products, therefore yielding unique and immediate benefits.
Claims7
1) A compound is added to lead bullion to react with amphoteric p-block elements to form Lewis bases.
2) Separation occurs at the liquid/liquid (or metal/slag) interface at a temperature less than 850° F.
3) The resulting Razor Process™ Slag layer, then incorporates the metal salts of amphoteric p-block elements.
4) The admixed amphoteric Lewis Acid is then reduced by the impurities removed from the lead bullion.
5) The precise stoichiometric amount of amphoteric Lewis Acid is added to preferentially remove the lighter amphoteric elements.
6) There is low potential for reversible reaction at the temperatures involved, thus allowing for process flexibility and reuse of the molten slag until the level of amphoteric p-block element impurities reaches a concentration greater than 10% in the Razor Process™ Slag melt layer. At this concentration the melt is removed and delivered to subsequent processing.
7) The entire Razor Process™ takes approximately six hours from start to finish, which is much less time than the traditional refining and separation processes, which typically takes approximately eighteen hours from start to finish.
Dependencies are inferred from the claim text.