A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxide film having an atomic ratio in a range of Si:O:C=100:140 to 170:20 to 40, peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1060 to 1090 cm−1, a film density in a range of 2.6 to 2.8 g/cm3 and a distance between grains of 30 nm or shorter, on a substrate film, using either of silicon having a sintered density of 80% or higher or silicon monoxide having a sintered density of 80% or higher as a target, in the presence of an oxygen gas by a sputtering method.