Abstract
A process for laser cutting a workpiece comprising the steps of providing a fiber-type laser resonator; providing a workpiece to be cut having a thickness of at least 1 mm; generating a laser beam using the laser resonator; focusing the laser beam in several distinct focus points, at least one of said focus points being focused in the thickness of the workpiece to be cut; and cutting said workpiece at a speed of at least 20 m/min.
Claims30
A process for laser cutting a workpiece, said process comprising the steps of:
- a. providing a fiber-type laser resonator;
- b. providing a workpiece to be cut having a thickness of at least 1 mm;
- c. generating a laser beam of at least 0.3 kW using the laser resonator;
- d. focusing the laser beam in several distinct focus points with at least one of said focus points being focused in the thickness of the workpiece to be cut;
- e. cutting said workpiece with said focused laser beam at a cutting speed of at least 20 m/min.
A process for laser cutting a workpiece, said process comprising the steps of:
- i. providing a fiber-type laser resonator comprises one or several ytterbium-comprising fibers;
- ii. providing a workpiece to be cut having a thickness of at least 1.3 mm;
- iii. generating a laser beam having a laser power of at least 1 kW using the laser resonator;
- iv. focusing the laser beam in two distinct focus points in the thickness of the workpiece to be cut;
- and
- v. cutting said workpiece with said focused laser beam at a cutting speed of at least 23 m/min.
A process for laser cutting a workpiece, said process comprising the steps of:
- i. providing a fiber-type laser resonator comprises one or several ytterbium-comprising fibers;
- ii. providing a workpiece to be cut made of steel, stainless steel, titanium, titanium alloy, aluminum or aluminum alloy and having a thickness of at least 1.3 mm;
- iii. generating a laser beam having a laser power of at least 2 kW and having a wavelength of from between 0.8 and 1.3 μm using the laser resonator;
- iv. focusing by means of a ZnS-comprising lens, the laser beam in two distinct focus points, at least one of said focus points being focused in the thickness of the workpiece to be cut;
- and
- v. cutting said workpiece with said focused laser beam at a cutting speed of at least 23 m/min.
A process for laser cutting a workpiece, said process comprising the steps of:
- i. providing a fiber-type laser resonator comprises one or several ytterbium comprising fibers;
- ii. providing a workpiece to be cut made of steel, stainless steel, titanium, titanium alloy, aluminum or aluminum alloy and having a thickness of at least 1.4 mm;
- iii. generating a laser beam having a laser power of at least 2 kW and having a wavelength of about 1.07 μm using the laser resonator;
- iv. focusing by means of a ZnS-comprising lens, the laser beam in two distinct focus points in the thickness of the workpiece to be cut;
- and
- v. cutting said workpiece with said focused laser beam at a cutting speed of at least 23 m/min.
Dependencies are inferred from the claim text.