The present invention relates to a zero-waste process for extraction of alumina from different types of bauxite ores and red mud residues and of titanium dioxide from ilmenite. Iron oxide is first reduced to metallic iron above the melting point of C-saturated cast iron alloy which yields a high-C iron alloy and an Al and Ti metal oxide rich slag which is then treated with alkali carbonate to form alkali aluminates and titanates. The alkali aluminates are separated by water leaching from which the hydroxide of alumina is precipitated by bubbling CO2. The residue from water leaching is treated with sulphuric acid and TiO2 is precipitated via a hydrolysis route. The process recovers most of the metal values and generates only small quantities of silicious residues at pH4-5 which can be used for soil conditioning. The present also relates to a method for selective separation of TiO2-rich oxides from titaniferrous ore/residue materials via oxidative roasting in the presence of alkali carbonate or carbonates followed by aqueous leaching of the roasted material and selective precipitation of TiO2 under controlled condition below pH=4.
A process for recovering at least one metal oxide from a titaniferrous or aluminaferrous mixture comprising:
A method for recovering titanium dioxide from a titanium oxide-containing composition comprising:
A process for the extraction of metal oxides, which comprises the steps of: