A process for production of an antistatic polyester false twisted yarn, characterized by simultaneous stretching and false twisting of an unstretched filament with a birefringence of 0.02-0.05, obtained by melt spinning of an aromatic polyester composition comprising (a) a polyoxyalkylene-based polyether and (b) an organic ionic compound that is substantially non-reactive with aromatic polyesters, wherein at least 75 mol % of the repeating units are ethylene terephthalate units, under conditions satisfying all of the following (a) to (d):
- (a) the false twisting tool used is a three-axis friction disc type wherein the material of the lowermost disc positioned at the untwisting section is ceramic, the contact length between that disc and the running yarn is 2.5-0.5 mm, and the diameter of the disc is 90-98% of the diameter of the disc immediately above it;
- (b) the false twisting temperature is 170° C.-300° C;
- (c) the draw ratio during false twisting is 1.4-2.4;
- and
- (d) the number of false twists T (/m) is 15,000/Y1/2≦T≦35,000/Y1/2, with respect to the size (Y dtex) of the false twisted yarn.