Abstract
Injection molded articles having large, thin sections are prepared by injection molding of a composition that includes specific amounts of poly(arylene ether) and a rubber-modified polystyrene. The specific component amounts provide the composition with a shear thinning index of 6 to 17 measured at a temperature of 260 to 300° C. and shear rates of 100 and 10,000 second−1.
Claims41
An injection molded article,
- wherein a portion of the injection molded article comprises
- a first dimension of at least 10 centimeters,
- a second dimension of at least 10 centimeters, and
- a third dimension of less than 1 centimeter;
- wherein the injection molded article is a product of injection molding an injection molding composition comprising
- 30 to 60 weight percent of a poly(arylene ether) having an intrinsic viscosity of 0.3 to 0.55 deciliter/gram measured at 25° C. in chloroform,
- 20 to 60 weight percent of a rubber-modified polystyrene, and
- 10 to 20 weight percent of a triaryl phosphate that is a liquid at one atmosphere and at least one temperature in the range 25 to 50° C.;
- wherein all weight percents are based on the total weight of the injection molding composition;
- and
- wherein the injection molding composition has a shear thinning index of 6 to 17 measured at shear rates of 100 and 10,000 second−1 at a temperature of 260 to 300° C. according to ASTM D3835.
8 more elements
A method of injection molding, comprising:
- injection molding an injection molding composition to form an injection molded article;
- wherein a portion of the injection molded article comprises
- a first dimension of at least 10 centimeters,
- a second dimension of at least 10 centimeters, and
- a third dimension of less than 1 centimeter;
- wherein the injection molded article is a product of injection molding an injection molding composition comprising
- 30 to 60 weight percent of a poly(arylene ether) having an intrinsic viscosity of 0.3 to 0.55 deciliter/gram measured at 25° C. in chloroform,
- 20 to 60 weight percent of a rubber-modified polystyrene, and
- 10 to 20 weight percent of a triaryl phosphate that is a liquid at one atmosphere and at least one temperature in the range 25 to 50° C.;
- wherein all weight percents are based on the total weight of the injection molding composition;
- and
- wherein the injection molding composition has a shear thinning index of 6 to 17 measured at shear rates of 100 and 10,000 second−1 at a temperature of 260 to 300° C. according to ASTM D3835.
9 more elements