Abstract
Nanoparticles having a mean particle size of less than about 25 nanometers and a mean pore size of less than 10 nanometers, and a mean surface area of at least 500 m2/g; nanoporous films of such nanoparticles; and composites and devices containing such nanoparticles and nanoporous films.
Claims32
A nanoporous film comprising:
- organosilica nanoparticles having a mean particle size of less than about 25 nanometers and a mean pore size of less than 10 nanometers;
- wherein the film has a surface area of at least 500 m2/g and a porosity of at least about 50% by volume.
A composite comprising:
- a substrate;
- a nanoporous film on the substrate, the nanoporous film comprising organosilica nanoparticles having a mean particle size of less than about 25 nanometers and a mean pore size of less than 10 nanometers;
- wherein the film has a surface area of at least 500 m2/g and a porosity of at least about 50% by volume.
A process for the preparation of a nanoporous film comprising nanoparticles, the process comprising:
- forming a solution of a nanoparticle precursor in a mixed solvent system comprising a first solvent and a second solvent, wherein the first solvent is different from the second solvent, wherein the second solvent has a boiling point which is greater than a boiling point of the first solvent, and wherein the nanoparticle precursor has a greater solubility in the first solvent than in the second solvent;
- removing at least 50% of the first solvent;
- depositing the solution as a film onto a substrate;
- and
- calcining the deposited film at a temperature of at least 200° C. to remove the second solvent from the film to form a nanoporous, nanoparticulate film having a thickness of less than 3 microns, a surface area of at least 500 m2/g, a refractive index of less than 1.33, a dielectric constant of less than 2, and a porosity of at least about 50% by volume.
2 more elements
A nanoparticulate mass comprising:
- organosilicate nanoporous nanoparticles having a mean particle size of less than about 25 nanometers, a mean pore size of less than 10 nanometers, and a mean surface area of at least 500 m2/g.
A waveguide comprising:
- at least two spaced-apart opposed surfaces defining a channel therebetween;
- a waveguide inlet;
- and
- a film on each of the two spaced-apart opposed surfaces wherein the film comprises organosilica nanoparticles having a mean particle size of less than about 25 nanometers and a mean pore size of less than 10 nanometers;
- wherein the film has a surface area of at least 500 m2/g and a porosity of at least about 50% by volume;
- the film has a thickness of less than about 3 microns;
- the film has a dielectric constant of less than 2;
- and
- the film has a refractive index of less than 1.33.
6 more elements
Dependencies are inferred from the claim text.