Pure ar gas shielded welding mig flux-cored wire and mig arc welding method
AssigneeKabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsReiichi SUZUKI, Yu UMEHARA, Toshihiko NAKANO
Life of this patent
Estimating the term…
Loading patent…
AssigneeKabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsReiichi SUZUKI, Yu UMEHARA, Toshihiko NAKANO
Estimating the term…
A pure Ar-MIG welding wire for welding steel according to the present invention is formed of a flux-cored wire. The flux-cored wire is formed in the manner that a formation formed by welding a carbon steel hoop into a pipe shape or a seamless pipe is used as an outer sheath, the outer sheath is filled with a flux, and a wire drawing process is performed. The flux accounts for 7 to 27 mass % of the total wire mass. The wire contains graphite in the amount of 0.16 to 2.00 mass % on the basis of the total wire mass and iron powder in the amount of 20 mass % on the basis of the total flux mass. According to the construction, neither expensive metal resource nor a greenhouse effect gas is used, slag and fume generation is inhibited, and a weld joint having a high static tensile strength and fatigue strength can be obtained.
A flux-cored wire to be used for MIG welding using a pure Ar shielding gas and to be formed with a steel outer sheath filled with a flux, the wire comprising in the flux,