Supported Metal Alkyl Compound And Its Preparation
AssigneeBasell Polyolefine GmbH
InventorsShahram Mihan, Rosendorfer Philipp, Rainer Karer, Martin Schneider, Peter Eck
Life of this patent
Estimating the term…
Abstract
Pulverulent solid which consists essentially of at least one metal alkyl compound bound chemically and/or physically to a finely divided, porous, mechanically stable and chemically inert support, has a proportion by weight of metal alkyl compound of at least 5% by weight, based on the support, and has an angle of repose, determined in accordance with ISO 4324, of up to 48°. The solid allows trouble-free metering as active component into a reactor.
Claims12
A pulverulent solid consisting essentially of at least one metal alkyl compound bound chemically and/or physically to a finely divided, porous, mechanically stable and chemically inert support and which has a proportion by weight of metal alkyl compound of at least 5% by weight, based on the support, and an angle of repose, determined in accordance with ISO 4324, of up to 48°.
A process for preparing a pulverulent solid consisting essentially of at least one metal alkyl compound bound chemically and/or physically to a finely divided, porous, mechanically stable and chemically inert support having an original water content, and which has a proportion by weight of metal alkyl compound of at least 5% by weight, based on the support, and an angle of repose, determined in accordance with ISO 4324, of up to 48°,
- the process comprising the steps:
- drying the support to a water content of less than 3% by weight if the original water content is at least 3% by weight;
- bringing the metal alkyl compound into contact with the support in an inert solvent having a boiling point of less than 30° C.;
- and
- removing the solvent from the pulverulent solid.
A process for preparing homopolymers and copolymers of α-olefins in a gas-phase fluidized-bed reactor, in which the α-olefin is (co)polymerized in a polymerization zone of the gas-phase fluidized-bed reactor at from 30 to 125° C. and pressures of from 1 to 100 bar in the gas phase in a mixed bed of finely divided polymer in the presence of at least one catalyst comprising a transition metal and in the presence of a pulverulent solid, and the resulting (co)polymers are discharged from the reactor, wherein the pulverulent solid consists essentially of at least one metal alkyl compound bound chemically and/or physically to a finely divided, porous, mechanically stable and chemically inert support and which has a proportion by weight of metal alkyl compound of at least 5% by weight based on the support, and an angle of repose, determined in accordance with ISO 4324, of up to 48°.
Dependencies are inferred from the claim text.