Time-delayed activation of zeolite heating
AssigneeHoneywell International Inc.
InventorsMARK R. WHEELER, Milton E. McDonnell, Maria M. Higuera, Michael Jablon, Richard B. Heath, Lee R. Mores
Life of this patent
Estimating the term…
Abstract
The invention relates to zeolite particles which are at least partially coated with a coating that is capable of delaying the release of heat from the zeolite particles upon contact with water over time. The coating effectively at least partially blocks the pore structure of the zeolite particle from contact with water, thereby delaying contact between water and the zeolite, and prolonging the warming effect caused by such contact.
Claims30
A time-delayed heat-release coated zeolite particle comprising a zeolite particle at least partially coated with a coating comprising a mixture of:
- a) at least one water-soluble component which is at least partially soluble in water at temperatures of from about 15° C. to about 25° C.;
- and
- b) at least one water-insoluble component which is substantially insoluble in water at temperatures of from about 15° C. to about 25° C.;
- wherein the coating has a melting temperature of from about 45° C. to about 120° C., and wherein the coating is capable of dissolving in water at temperatures of from about 15° C. and 25° C. in an amount sufficient to at least partially expose the zeolite particle to the water.
A process for heating a fluid composition which comprises:
- I) providing a fluid composition which comprises a plurality of time-delayed heat-release coated zeolite particles, each comprising a zeolite particle at least partially coated with a coating comprising a mixture of:
- a) at least one water-soluble component which is at least partially soluble in water at temperatures of from about 15° C. to about 25° C.;
- and
- b) at least one water-insoluble component which is substantially insoluble in water at temperatures of from about 15° C. to about 25° C.;
- wherein the coating has a melting temperature of from about 45° C. to about 120° C., and wherein the coating is capable of dissolving in water at temperatures of from about 15° C. and 25° C. in an amount sufficient to at least partially expose the zeolite particle to the water;
- and
- II) contacting the fluid composition with water to thereby at least partially dissolve the coatings of the time-delayed heat-release coated zeolite particles, thus exposing the zeolite particles to the water such that the zeolite particles generate heat.
A process for forming time-delayed heat-release coated zeolite particles comprising:
- I) forming a coating composition for coating zeolite particles, which comprises a mixture of:
- a) at least one water-soluble component which is at least partially soluble in water at temperatures of from about 15° C. to about 25° C.;
- and
- b) at least one water-insoluble component which is substantially insoluble in water at temperatures of from about 15° C. to about 25° C.;
- II) heating the coating composition during or after step I, thereby forming a molten coating composition;
- III) coating zeolite particles with the molten coating composition;
- and
- IV) cooling the molten coating composition to thereby form time-delayed heat-release coated zeolite particles having a coating, which coating has a melting temperature of from about 45° C. to about 120° C., and which coating is capable of dissolving in water at temperatures of from about 15° C. and 25° C. in an amount sufficient for the zeolite particles to be at least partially exposed to the water.
A time-delayed heat-release coated zeolite particle comprising a zeolite particle partially coated with a water-insoluble coating, which coating comprises:
- a water-insoluble component comprising a crystalline or semicrystalline material having a glass transition temperature of about 40° C. or greater, and a melting point of about 150° C. or lower.
A process for heating a fluid composition which comprises:
- I) providing a fluid composition which comprises a plurality of time-delayed heat-release coated zeolite particles, each comprising a zeolite particle partially coated with a water-insoluble coating which comprises a water-insoluble component comprising a crystalline or semicrystalline material having a glass transition temperature of about 40° C. or greater, and a melting point of about 150° C. or lower;
- and
- II) contacting the fluid composition with water to thereby partially expose the zeolite particles to the water such that the zeolite particles generate heat.
A process for forming time-delayed heat-release coated zeolite particles comprising:
- I) forming a water-insoluble coating composition for coating zeolite particles, which comprises a water-insoluble component comprising a crystalline or semicrystalline material having a glass transition temperature of about 40° C. or greater, and a melting point of about 150° C. or lower;
- II) heating the coating composition during or after step I, thereby forming a molten water-insoluble coating composition;
- III) coating zeolite particles with the molten water-insoluble coating composition;
- and
- IV) cooling the molten coating composition to thereby form time-delayed heat-release coated zeolite particles having a water-insoluble coating, which coating is sufficient to partially expose the zeolite particles to water.
Dependencies are inferred from the claim text.