Shaped Steel Excellent in Fire Resistance and Producing Method Therefor
AssigneeNippon Steel Corporation
InventorsSuguru Yoshida, Kazuhiko Eda, Hiroshi Kita
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Steel Corporation
InventorsSuguru Yoshida, Kazuhiko Eda, Hiroshi Kita
Estimating the term…
A shaped steel, such as H-shaped steel, excellent in fire resistance, where a flange portion has 50% or more of a ratio of strength, 80% or less of yield ratio, and 100 J or more of impact strength of Charpy impact test at 0° C., wherein the ratio of strength=(proof stress of 0.2% at 600° C.)/(yield strength at room temperature), and a producing method thereof are provided. The shaped steel comprises in mass percent (%): C: 0.03-0.15; Mo: 0.1-0.6; V≦0.35; and N: 0.002-0.012, and the balance being iron and residual impurities, wherein (x) a mol fraction of precipitate of alloy carbides and alloy carbonitrides at 600° C. is 0.3% or more, and (y) the ratio of the mol fraction of precipitate of alloy carbides and alloy carbonitrides at 300° C. to the mol fraction of precipitate of alloy carbides and alloy carbonitrides at 600° C. is 2.0 or less.
A shaped steel, comprising in mass percent (%):
Dependencies are inferred from the claim text.