Cutter composed of ni-cr alloy
AssigneeKabushiki Kaisha Toshiba
InventorsTomohisa ARAI, Takashi Rokutanda, Tadaharu Kido
Life of this patent
Estimating the term…
Abstract
A cutter is composed of a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6.0 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more. This Ni—Cr alloy provides a cutter produced with a superior workability and by a significantly simplified process, having a low deterioration in the hardness even when heated in use, having excellent corrosion resistance and low-temperature embrittlement resistance, and satisfactorily maintaining the cutting performance for a long time.
Claims21
A cutter comprising a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more, and wherein the chromium is partly replaced with at least one element selected from Zr, Hf, V, Ta, Mo, W and Nb, the total replacement ratio of Zr, Hf, V and Nb is one mass percent or less, the replacement ratio of Ta is two mass percent or less, and the total replacement ratio of Mo and W is 10 mass percent or less.
A cutter comprising a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more, and wherein the total replacement ratio of a plurality of the elements represented by a formula (Zr+Hf+V+Nb)×10+Ta×5+(Mo+W) is 10 mass percent or less, wherein the name of elements Zr, Hf, Ta, Mo, W and Nb represents the replacement ratio of each element, the elements partly replacing the chromium.
A cutter comprising a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more, and wherein the aluminum is partly replaced with 1.2 mass percent or less of Ti.
A cutter comprising a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more, and wherein the nickel is partly replaced with 5 mass percent or less of Fe.
A cutter comprising a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more, and wherein the Ni—Cr alloy further comprises:
- 0.1 mass percent or less of C;
- 0.05 mass percent or less of Mn;
- 0.005 mass percent or less of P;
- 0.005 mass percent or less of O;
- 0.003 mass percent or less of S;
- 0.02 mass percent or less of Cu;
- and
- 0.05 mass percent or less of Si;
- as the impurities and the additional trace elements,
- the total content of P, O, and S is 0.01 mass percent or less, and the total content of Mn, Cu, and Si is 0.05 mass percent or less.
A cutter comprising a Ni—Cr alloy containing from 32 to 44 mass percent of Cr, from 2.3 to 6 mass percent of Al, the balance being Ni, impurities, and additional trace elements and having a Rockwell C hardness of 52 or more, and wherein the Ni—Cr alloy further comprises:
- 0.025 mass percent or less of Mg;
- 0.02 mass percent or less of Ca;
- 0.03 mass percent or less of B;
- and
- 0.02 mass percent or less of rare earth elements including Y;
- as the impurities and the additional trace elements, and the total content of Mg, Ca, and B is 0.03 mass percent or less (but when the total content of Mg, Ca, and B is 0.015 mass percent or more, the total content of P, O, and S is 0.003 mass percent or less and the total content of Mn, Cu and Si is 0.03 mass percent or less).
A method of manufacturing a cutter composed of Ni—Cr—Al alloy, the method comprising the steps of:
- preparing an alloy ingot by melting steels;
- conducting hot working and cold working to the alloy ingot thereby to form a plate;
- performing solution heat treatment to the plate at a temperature of 1,000° C. to 1,300° C. in argon atmosphere, nitrogen atmosphere, or in air;
- quenching the plate at a cooling rate higher than oil quenching to form a blank plate;
- performing aging treatment to the blank plate at a temperature of 550° C. to 800° C.;
- and
- forming a mirror-finished surface onto the blank plate by final polishing with a polisher
Dependencies are inferred from the claim text.