Abstract
The invention concerns a method for preparing glass from raw materials in powder form in a furnace comprising three side walls, a roof, an upstream pinion and at least one air injector associated with a gas or liquid fuel injector, at least one of said injectors being arranged in said side walls, in said roof or in said upstream pinion. Said method includes the following steps: injecting air and gas or liquid fuel through said injectors, at least one flame being generated immediately proximate the zone where said raw materials in powder form cover the glass solution.
Claims12
1:
- A process for preparing glass from pulverulent batch materials in a furnace comprising sidewalls, a crown, an end wall and at least one air injector combined with at least one gaseous or liquid fuel injector, at least one of said injectors being placed in said sidewalls, in said crown or in said end wall, said process comprising the steps of injecting air and gaseous or liquid fuel through said injectors to generate flames, whereby each flame thus generated is generated in the immediate vicinity of the zone where said pulverulent batch materials cover the glass bath.
The process as claimed in claim 1, characterized in that the furnace comprises at least one overhead burner, of which the oxidizer is air, and at least one regenerator or recuperator.
The process as claimed in claim 1, characterized in that the injection of air and of gaseous or liquid fuel is carried out via a burner comprising at least one approximately cylindrical inner duct for the fuel and an outer duct for the air that is concentric to the inner duct.
The process as claimed in claim 1, characterized in that the fuel and the air are injected from different places in the furnace.
The process as claimed in claim 1, characterized in that the specific impulse of the combination of injectors is between 2 and 4 N/MW.
The process as claimed in claim 1, characterized in that the fuel and air flows exiting the injectors are not laminar.
The process as claimed in claim 1, characterized in that the air used as an oxidizer is preheated to a temperature of at least 500° C. before entering the furnace.
The process as claimed in claim 1, characterized in that the air is introduced under substoichiometric conditions relative to the fuel in order to produce a glass whose redox is greater than 0.3.
The process as claimed in claim 1, characterized in that the chemical composition of the glass comprises more than 3% by weight of boron oxide and/or more than 12% by weight of alkali metal oxides.
The process as claimed in claim 1, characterized in that the glass produced contains less than 2% by weight of alkali metal oxides.
A process for preparing glass from pulverulent batch materials in a furnace comprising sidewalls, an end wall and at least one burner placed in said sidewalls or in said end wall, said process comprising the steps of injecting an oxidizer and gaseous or liquid fuel through or in combination with said at least one burner, whereby a flame is generated in the immediate vicinity of the zone where said pulverulent batch materials cover the glass bath.
Dependencies are inferred from the claim text.