Polyester/polycarbonate blends with reduced yellowness
AssigneeEastman Chemical Company
InventorsVALERIE ADAMS, EMMETT CRAWFORD, MICHAEL DONELSON, DOUGLAS MCWILLIAMS
Life of this patent
Estimating the term…
Abstract
Thermoplastic compositions of polyester/polycarbonate blends have reduced yellowness and improved thermal and melt stability when the polyester is produced with a reduced level of a titanium-containing catalyst in an amount of from about 1 to about 30 ppm elemental titanium, with ppm based on the total weight of the polyester.
Claims11
1-42. (canceled)
A polyester composition having an inherent viscosity of from about 0.6 to about 1.2 dl/g measured at 25° C. in a solvent mixture consisting of 60% by weight phenol and 40% by weight tetrachloroethane and the polyester comprising:
- (a) an acid component comprising repeat units from terephthalic acid, isophthalic acid, and mixtures thereof;
- (b) a diol component comprising repeat units from about 40 to 100 mole percent 1,4-cyclohexanedimethanol and about 0 to about 60 mole percent ethylene glycol;
- and
- (c) catalyst residues consisting essentially of (i) a titanium-containing catalyst compound in an amount of about 1 to about 15 ppm elemental titanium, (ii) a pre-polycondensation phosphorus-containing compound in an amount of about 45 to about 100 ppm elemental phosphorus, (iii) from about 1 to about 5 ppm of at least one copolymerizable compound of a 6-arylamino-1-cyano-3H-dibenz[f,ij]isoquinoline-2,7-dione or a 1,4-bis(2,6-dialkylanilino) anthraquinone in combination with at least one bis anthraquinone or bis anthrapyridone(6-arylamino-3H-dibenz[f,ij]isquinoline-2,7-done) compound, wherein the compounds contain at least one polyester reactive group, and (iv) optionally, an ester exchange catalyst in an amount of from about 10 to about 65 ppm of an active element utilized when the acid component is derived from a diester of the dicarboxylic acid;
- wherein the acid component is based on 100 mole percent and the diol component is based on 100 mole percent and ppm are based on the total weight of the polyester.
In a thermoplastic composition comprising a miscible blend of:
- (a) about 1 to about 99 weight percent of a polyester comprising:
- (i) an acid component comprising repeat units from about 80 to 100 mole percent of terephthalic acid, isophthalic acid, naphthalenedicarboxylic acid, 1,4-cyclohexanedicarboxylic acid or mixtures thereof and from 0 to about 20 mole percent of other dicarboxylic acid units having from about 4 to about 40 carbon atoms, wherein the total mole percent of the acid component is equal to 100 mole percent,
- and
- (ii) a diol component comprising repeat units from about 40 to 100 mole percent of 1,4-cyclohexanedimethanol, from 0 to about 60 mole percent of ethylene glycol, and from 0 to about 20 mole percent of other diol units having from 3 to about 12 carbon atoms, wherein the total mole percent of diol component is equal to 100 mole percent;
- and
- (b) about 99 to about 1 weight percent of a polycarbonate of 4,4-isopropylidenediphenol;
- the improvement comprising the polyester comprising:
- (i) catalyst residues of a titanium-containing catalyst compound in an amount of from about 1 to about 20 ppm elemental titanium;
- (ii) catalyst residues of a pre-polycondensation phosphorus-containing compound in an amount of from about 1 to about 150 ppm elemental phosphorus;
- (iii) from about 1 to about 10 ppm of at least one copolymerizable compound of a 6-arylamino-1-cyano-3H-dibenz[f,ij]isoquinoline-2,7-dione or a 1,4-bis(2,6-dialkylanilino) anthraquinone in combination with at least one bis anthraquinone or bis anthrapyridone(6-arylamino-3H-dibenz[f,ij]isquinoline-2,7-done) compound, wherein the compounds contain at least one polyester reactive group;
- and
- (iv) optionally, an ester exchange catalyst in an amount of from about 1 to about 150 ppm of an active element utilized when the acid component is derived from a diester of the dicarboxylic acid, with ppm based on the total weight of the polyester, and the blend further comprising from about 0.01 to about 0.35 weight percent of a post-polycondensation phosphorus-containing compound, based on the total weight of the blend, having one of the formulas (a)-(e):
- wherein each of R1, R2, and R3 represents a hydrogen atom, an alkyl group containing 1 to 20 carbon atoms, an aryl group containing 6 to 20 carbon atoms, an arylalkyl group containing 7 to 20 carbon atoms, or an OR group in which R is a hydrogen atom, an alkyl group containing 1 to 20 carbon atoms, an aryl group containing 6 to 20 carbon atoms, and arylalkyl group containing 7 to 20 carbon atoms;
- R1, R2, and R3 may be different from each other, or at least two of R1, R2, and R3 may be the same, or at least two of R1, R2, and R3 may form a ring, and metal salts of these phosphorous compounds;
- (c)
- wherein R1 represents a divalent alkyl group having 2-12 carbon atoms or a divalent aryl group having 6-15 carbon atoms;
- R2 and R3 are monovalent alkyl groups having 2-18 carbon atoms, or a monovalent aryl or substituted aryl group having 6 to 15 carbons;
- wherein R1 represents a divalent alkyl or poly(alkylene oxide) groups having 2-12 carbon atoms or a divalent aryl or substituted aryl group having 6-15 carbon atoms;
- and
- wherein R1 and R2 represent monovalent alkyl groups having 2-18 carbon atoms, or a monovalent aryl or substituted aryl groups having 6-15 carbon atoms.
Dependencies are inferred from the claim text.