Methods of preparing silica sols, and stable high-solids silica sols prepared thereby
AssigneeH.C. Starck GmbH
InventorLothar Puppe
Life of this patent
Estimating the term…
Abstract
Methods comprising: (a) providing a silica sol having a BET surface area of 15 to 1000 m2/g and a solids content of up to 45% by weight of silicon dioxide, based on the silica sol; (b) mixing the silica sol and an anionic polyether carboxylate to form a mixture, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.01 to 10% by weight, based on the mixture; and (c) concentrating the mixture to form a concentrated mixture having a solids content of 20 to 70% by weight of silicon dioxide, based on the concentrated mixture; and the concentrated sols prepared thereby.
Claims15
A method comprising:
- (a) providing a silica sol having a BET surface area of 15 to 1000 m2/g and a solids content of up to 45% by weight of silicon dioxide, based on the silica sol;
- (b) mixing the silica sol and an anionic polyether carboxylate to form a mixture, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.01 to 10% by weight, based on the mixture;
- and (c) concentrating the mixture to form a concentrated mixture having a solids content of 20 to 70% by weight of silicon dioxide, based on the concentrated mixture.
A method comprising:
- (a) providing a silica sol having a BET surface area of 100 to 600 m2/g, wherein the silica sol comprises silicon dioxide particles having a mean particle diameter of 3 nm to 250 nm and a solids content of up to 45% by weight of silicon dioxide, based on the silica sol;
- (b) mixing the silica sol and an anionic polyether carboxylate to form a mixture, wherein the anionic polyether carboxylate is mixed with the silica sol in an amount of 0.05 to 10% by weight, based on the mixture;
- and (c) concentrating the mixture to form a concentrated mixture having a solids content of 40 to 60% by weight of silicon dioxide, based on the concentrated mixture.
A concentrated silica sol mixture comprising:
- (a) silicon dioxide particles having a mean particle diameter of 3 nm to 250 nm and having a BET surface area of 15 to 1000 m2/g;
- and (b) an anionic polyether carboxylate;
- wherein the concentrated silica sol mixture has a solids content of 20 to 70% by weight of silicon dioxide, based on the concentrated mixture.
Dependencies are inferred from the claim text.