Method of producing semiconductor device
AssigneeFujitsu Limited
InventorsKazuo Kawamura, Satoshi Inagaki, Takashi Saiki, Ryou Nakamura
Life of this patent
Estimating the term…
Abstract
A method of producing a semiconductor device is disclosed that is able to reduce fluctuations of a sheet resistance of a silicide layer in the semiconductor device formed by a salicide process. When depositing a titanium nitride film on a cobalt film in the salicide process, the thickness of the titanium nitride film is set to be sufficiently small so that a nano-grain structure or an amorphous structure is formed in the titanium nitride film. In the titanium nitride film, the titanium composition is enriched.
Claims16
A method of producing a semiconductor device having a gate width less than 50 nm, comprising:
- a step of forming a poly-silicon gate electrode pattern having a gate width less than 50 nm on a semiconductor substrate;
- a step of forming a first diffusion region and a second diffusion region on two respective sides of the poly-silicon gate electrode pattern in the semiconductor substrate;
- a step of depositing a cobalt film on the semiconductor substrate so as to cover the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern;
- a step of depositing a titanium nitride film on the cobalt film;
- and
- a step of, after the step of depositing the titanium nitride film, inducing a reaction between the cobalt film and surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern so as to form a CoSi2 film;
- wherein the titanium nitride film is formed such that a crystal grain diameter of the titanium nitride film is less than a thickness of the titanium nitride film.
A method of producing a semiconductor device having a gate width less than 50 nm, comprising:
- a step of forming a poly-silicon gate electrode pattern having a gate width less than 50 nm on a semiconductor substrate;
- a step of forming a first diffusion region and a second diffusion region on two respective sides of the poly-silicon gate electrode pattern in the semiconductor substrate;
- a step of depositing a cobalt film on the semiconductor substrate so as to cover the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern;
- a step of depositing a titanium nitride film on the cobalt film;
- and
- a step of, after the step of depositing the titanium nitride film, inducing a reaction between the cobalt film and surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern so as to form a CoSi2 film;
- wherein the titanium nitride film is formed to have an amorphous phase.
A method of producing a semiconductor device having a gate width less than 50 nm, comprising:
- a step of forming a poly-silicon gate electrode pattern having a gate width less than 50 nm on a semiconductor substrate;
- a step of forming a first diffusion region and a second diffusion region on two respective sides of the poly-silicon gate electrode pattern in the semiconductor substrate;
- a step of depositing a cobalt film on the semiconductor substrate so as to cover the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern;
- a step of depositing a titanium nitride film on the cobalt film, a composition of said titanium nitride film being denoted as TixNy (x+y=1);
- and
- a step of, after the step of depositing the titanium nitride film, inducing a reaction between the cobalt film and surfaces of the first diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern so as to form a CoSi2 film;
- wherein the composition of the titanium nitride film satisfies x>y.
A semiconductor device, comprising:
- a semiconductor substrate;
- a poly-silicon gate electrode pattern having a gate width less than 50 nm formed on the semiconductor substrate with a gate insulating film in between;
- and
- a first diffusion region and a second diffusion region in the semiconductor substrate on two respective sides of the poly-silicon gate electrode pattern and on respective outer sides of sidewall insulating films of the poly-silicon gate electrode;
- wherein
- a CoSi2 film is formed on surfaces of the first-diffusion region, the second diffusion region, and the poly-silicon gate electrode pattern, and
- an atomic percentage of titanium in the CoSi2 film is in a range from 0.1% to 1%.
Dependencies are inferred from the claim text.