Atmospheric process and system for controlled and rapid removal of polymers from high aspect ratio holes
AssigneeJetek, Inc.
InventorsLynn Bollinger, Iskander Tokmouline
Life of this patent
Estimating the term…
Abstract
A system that generates an intense hot gas stream is described to etch a polymer on a substrate used in the manufacture of semiconductor and MEMS devices with no surface damage. The etching process is particularly useful to remove a polymer from relatively high aspect Height-to-Width and Width-to-Height ratio holes that can include trenches, having relatively large aspect ratios for removal of polymers used in connection with the manufacturing of microstructures.
Claims22
A method for making micro-structures in a substrate comprising the steps of:
- using a polymer to protect or support the micro-structures during fabrication;
- and
- removing the polymer after completion of fabrication by generating and directing a hot gas stream at the substrate containing the micro-structure devices.
A method for removing a polymer from a substrate having micro-structures that are filled with a polymer, comprising the steps of:
- directing an atmospheric hot gas stream having a heat flux in the range from about 106 to 108 W/m2 for a controlled rapid removal of a polymer from the micro-structures in the substrate;
- and
- varying the position on the substrate that is exposed to the hot gas to obtain a substantially uniform removal of polymer material from the micro-structures in the substrate.
A method for removing a polymer from a substrate having micro-structures that are filled with a polymer, the micro-structures having depth-width (D-W) or width-depth (W-D) aspect ratios of greater than 10 to 1, comprising the steps of:
- directing a hot gas stream at the substrate containing the micro-structure devices having D-W or W-D aspect ratios of greater than 10 to 1;
- and
- removing the polymer from the micro-structure devices having D-W or W-D aspect ratios of greater than 10 to 1.
A substrate having micro-structure devices having at least one depth-width (D-W) or width-depth (W-D) aspect ratio hole in which a polymer has been removed according to the following process:
- directing a hot gas stream at the substrate containing the micro-structure devices having the at least one D-W or W-D aspect ratio hole of greater than 10 to 1;
- and
- removing the polymer from the micro-structure devices having the at least one D-W or W-D aspect ratio hole of greater than 10 to 1.
Dependencies are inferred from the claim text.