Polymers having low levels of long chain branching and methods of making the same
AssigneeChevron Phillips Chemical Company LP
InventorsMax McDaniel, Kathy Collins, Elizabeth Benham, Paul DesLauriers
Life of this patent
Estimating the term…
Loading patent…
AssigneeChevron Phillips Chemical Company LP
InventorsMax McDaniel, Kathy Collins, Elizabeth Benham, Paul DesLauriers
Estimating the term…
Methods of producing a polymer include contacting at least one olefin with a catalyst prepared by contacting a support comprising alumina with a sulfating agent and with chromium. Polymer compositions produced in this manner may exhibit relatively low levels of long chain branching and relatively high molecular weights. In an embodiment, polymer compositions with a PDI in a range of from about 6 to about 15 have MW values greater than about 300,000 g/mol and Eo values less than about 1×106 Pa.s. The polymer compositions may further have Theological breadths greater than about 0.25 and relaxation times less than about 10 seconds.
A method of producing a polymer comprising contacting at least one olefin with a catalyst prepared by contacting a support comprising alumina with a sulfating agent and with chromium.
A polymer composition having a PDI in a range of from about 6 to about 15, a MW greater than about 300,000 g/mol, and an Eo less than about 1×106 Pa.s.
A polymer composition having a PDI in a range of from about 6 to about 15, a MW greater than about 500,000 g/mol, and an Eo less than about 5×106 Pa.s.
A polymer composition having a PDI in a range of from about 6 to about 15, a MW greater than about 300,000 g/mol and a relaxation time less than about 10 seconds.
A polymer composition having a PDI in a range of from about 6 to about 15, a MW greater than about 300,000 g/mol, and a rheological breadth greater than about 0.25.
A polymer composition made using a chromium-based catalyst, the polymer composition having a HLMI less than about 100 g/10 min and a Theological breadth greater than about 0.25.
A polymer composition comprising polyethylene and having a PDI in a range of from about 6 to about 15, a HLMI less than about 5 g/10 min, and an Eo less than about 1×106 Pa.s.
A polymer composition comprising polyethylene and having a PDI in a range of from about 6 to about 15, a HLMI less than about 2 g/10 min, and an Eo less than about 5×106 Pa.s.
Dependencies are inferred from the claim text.