Mesh suitable for use as a light attenuating screen and method for making the same
AssigneeXLScreen
InventorsPhilippe Christou, Martine Pellet, Alain Crouzet
Life of this patent
Estimating the term…
Abstract
A mesh suitable for use as a light attenuating screen is disclosed. The mesh may contain not less than two sheets of glass yarn, joined to form a mesh having a specific openness factor and coated with a polymer coating containing TiO2 particles, so that the glass yarn is separated from TiO2 particles by at least a portion of the polymer binder. A method for making a mesh suitable for use as a light attenuating screen is also disclosed.
Claims22
A mesh suitable for use as a light attenuating screen, said mesh comprising not less than two sheets of glass yarn, joined to one another to form a mesh with an openness factor and coated with a polymer coating containing TiO2 particles, the glass yarn being separated from the TiO2 particles by at least a portion of the polymer coating.
A method of making a mesh comprising not less than two sheets of glass yarn and having an openness factor, said method comprising the steps of:
- (i) applying a treatment (b) to the mesh by soaking the mesh in a first bath containing, in % of total dry weight:
- about 35 to about 55% of at least one vinyl binder;
- about 5 to about 25% of at least one polyurethane binder;
- about 20 to about 50% of a flame retardant;
- about 0.5 to about 3% of an anti-foaming agent;
- and
- 0 to about 0.5% of at least one pigment other than TiO2;
- wherein treatment (b) is applied to form a treatment layer (b) representing, as a percentage of dry weight, from about 6 to about 15% of a total weight of the mesh;
- and
- (ii) applying a treatment (c) to the mesh by soaking the mesh with treatment layer (b) in a second bath containing, in % of total dry weight:
- about 25 to about 45% of at least one vinyl binder;
- about 5 to about 25% of at least one polyurethane binder;
- about 10 to about 30% of a flame retardant;
- about 20 to about 40% of titanium dioxide;
- about 0.5 to about 3% of an anti-foaming agent;
- and
- 0 to about 0.5% of at least one pigment other than TiO2;
- wherein treatment (c) is applied to form a treatment layer (c) representing, as a percentage of dry weight, from about 4 to about 15% of a total weight of the mesh.
A mesh suitable for use as a light attenuating screen, said mesh comprising:
- not less than two sheets of glass yarn, joined to one another to form a mesh having an openness factor, a first side, and a second side opposite the first side;
- a first polymer coating on the first side of the mesh, said first polymer coating containing TiO2 particles, the glass yarn being separated from the TiO2 particles by at least a portion of the first polymer coating,
- wherein the second side of the mesh is substantially free of said first polymer coating.
Dependencies are inferred from the claim text.