Composite material
AssigneeUnited Technologies Corporation
InventorsForrest Goodson, Hugh Reynolds
Life of this patent
Estimating the term…
Abstract
A composite material and method of manufacture involve a mixture of an epoxy resin and a hardener being essentially free of methylenedianiline and vinylcyclohexene dioxide. A fiber reinforcement is located within the matrix. Advantageously, the matrix has a glass transition temperature of at least 250° F. dry, the resin has a pre-hardening mixed viscosity of 500-1500 cP at 75° F., and the composite material has, upon hardening, an interlaminar shear strength of at least 6.5 ksi dry at 75° F. and at least 3.5 ksi dry at 250° F.
Claims8
A composite material comprising:
- a matrix mixture of an epoxy resin and a hardener, the epoxy resin and hardener being essentially free of methylenedianiline (MDA) and vinylcyclohexene dioxide;
- and
- a fiber reinforcement within the matrix,
- wherein:
- the matrix has a glass transition temperature of at least 250° F. dry;
- and
- the resin has a pre-hardening mixed viscosity of 500-1500 cP at 75° F.;
- and
- the composite material has, upon hardening, an interlaminar shear strength of at least 6.5 ksi dry at 75° F. and at least 3.5 ksi dry at 250° F.
A method for manufacturing a composite material comprising:
- forming a blend of:
- a resin selected from the group consisting of low viscosity bisphenol A/epichlorohydrin resins, low viscosity cycloaliphatic resins, and low viscosity tetra functional epoxy resins;
- and
- a hardener selected from the group consisting of liquid aromatic amine hardeners effective to provide glass transition temperatures in excess of 250° F., the blend being essentially free of methylenedianiline (MDA) and vinylcyclohexene dioxide;
- embedding fiber reinforcement in the blend;
- and
- curing the fiber-reinforced blend to form the composite material having an interlaminar shear strength of at least 6.5 ksi dry at 75° F. and 3 ksi dry at 250° F. and a fiber tensile strength of at least 650 ksi in a filament-wound pressure vessel at 75° F.
Dependencies are inferred from the claim text.