Back to results
US 2004/0081824 A1Published application
Oxide coated cutting tool
AssigneeSandvik AB, Sandviken, Sweden.
InventorBjorn Ljungberg
Life of this patent
Estimating the term…
Abstract
A body is at least partially coated with one or more refractory layers of which at least one layer is of a fine grained κ-Al2O3. Said κ-Al2O3 layer has equiaxed grains with an average grain size of <0.5 μm. The Al2O3 layer also has at least one sublayer containing Al, Si and O. The fine grained κ-Al2O3 microstructure is obtained by periodically introducing a silicon halide, preferably SiCl4, during the Al2O3-process.
Claims10
A cutting tool comprising:
- a body of sintered cemented carbide, cermet or ceramic;
- and
- a hard and wear resistant coating applied on at least a functioning portion of a surface of the body, wherein said coating comprises a structure of one or more refractory layers of which at least one layer consists essentially of an equiaxed fine grained K-Al2O3 with a thickness of 0.5-25 μm and with a grain size of less than 0.5 μm, and said fine grained κ-Al2O3 layer comprises at least one sublayer with a thickness between 0.02 and 3 μm containing Al, Si and 0 with a Si concentration between 4-34 at %, Al concentration of 0-37 at % and 0 concentration of 60-67 at %.
A method of coating a body with at least one fine grained κ-Al2O3 layer, the method comprising:
- contacting the body with a reaction mixture comprising a hydrogen carrier gas, one or more halides of aluminium and a hydrolysing and/or oxidising agent at 800-1050 C;
- adding a sulphur agent to the reaction mixture to enhance the growth rate;
- and
- depositing a κ-Al2O3 layer comprising at least one silicon enriched sublayer by periodically introducing a silicon halide.
1 more element
Dependencies are inferred from the claim text.