Production of thin steel strip
OwnerLazar Strezov, Kannappar Mukunthan +2inventors
InventorsLazar Strezov, Kannappar Mukunthan, Walter Blejde, Rama Mahapatra
Life of this patent
Estimating the term…
Abstract
A cast carbon steel strip is prepared by continuously casting in a twin roll caster and cooling to transform the strip from austenite to ferrite at a temperature range between 400° C. and 850° C. at a cooling rate of not more than about 100° C./sec, such that the strip has a yield strength of greater than 450 MPa. The cast strip before cooling is passed through a hot rolling mill to reduce the thickness of strip by at least 15% and up to 50%.
Claims26
A cast steel strip prepared by a process comprising the steps of:
- supporting a casting pool of molten low carbon steel on a pair of chilled casting rolls forming a nip between them and continuously casting solidified strip of no more than 5 mm in thickness and including austenite grains by rotating the rolls in mutually opposite directions such that the solidified strip moves downwardly from the nip;
- passing the strip through a rolling mill in which it is hot rolled to produce a reduction in the strip thickness of at least 15%, and
- cooling the strip to transform the austenite to ferrite within a temperature range between 850° C. and 400° C. and at a cooling rate of more than about 100° C./sec.
A cast steel strip prepared by a process comprising the steps of:
- supporting a casting pool of molten low carbon steel on a pair of chilled casting rolls forming a nip between them and continuously casting solidified strip of no more than 5 mm in thickness and including austenite grains by rotating the rolls in mutually opposite directions such that the solidified strip moves downwardly from the nip;
- passing the strip through a rolling mill in which the strip is hot rolled to produce a reduction in the strip thickness of at least 15%;
- and
- continuously cooling the strip to transform the austenite to ferrite within a temperature range between 400° C. and 850° C. at a cooling rate of not less than 90° C./sec without inhibiting the cooling rate.