Abstract
The present invention concerns a method of improving the properties of powder metallurgically produced SMC compacted body consisting of a soft magnetic material of insulated powder particles and a lubricant, to a stress relieving heat treatment in a furnace until the component has reached a temperature of at least 400° C. in an oxygen containing atmosphere having a CO content is less than 0.25% by volume.
Claims6
Method of improving the properties of powder metallurgically produced SMC components by subjecting a compacted body consisting of a soft magnetic material of insulated powder particles and a lubricant, to a stress relieving heat treatment in a furnace until the component has reached a temperature of at least 400° C. in an oxygen containing atmosphere having a CO content less than 0.25% by volume.
Method according to any one of the claims 1-6 characterised in that the furnace temperature is set at a value above the maximum intended component temperature, that the temperature of the SMC compound is measured and that the heat treating cycle is terminated when the temperature of the component reaches the intended component temperature.
Dependencies are inferred from the claim text.