Spall propagation properties of case-hardened M50 and M50NiL bearings
AssigneeGeneral Electric Company
InventorsMark Alan Rhoads, Michael Gilbert Johnson, Jonothan Allen Scheetz
Life of this patent
Estimating the term…
Loading patent…
AssigneeGeneral Electric Company
InventorsMark Alan Rhoads, Michael Gilbert Johnson, Jonothan Allen Scheetz
Estimating the term…
A roller bearing that provides ball and roller bearing elements comprised of M50 steel and M50NiL steel having surface hardnesses above 60 HRC, and in the range of 65-72 HRC. The hardness in the surface region is achieved by nitriding the surface to achieve a high hardness and extended life. This improvement is brought about by controlling the microstructure of the alloy by minimizing the formation of retained austenite. The material is tempered as required. The surface is then nitrided, but the nitriding operation is carefully controlled to avoid the formation of intergranular nitrides. Because of the method used to prevent the formation of intergranular nitrides, some carbon may be present to prevent the surface of the steel from becoming depleted of carbon. The hardening element in this nitro-carburizing operation is nitrogen, which forms iron nitride as Fe3N or Fe4N intragranularly. The purpose of the carbon in the operation is to maintain the concentration of carbon in the surface of the bearing so that the properties are not altered by decarburizing the surface. Standard gaseous and plasma nitriding techniques also may be used for the nitriding operation.
A bearing material comprising:
A method of manufacturing a bearing element from a martensitic steel, the bearing element characterized by a surface region with a hardness in the range of about 64-72 HRC, the surface region being case-hardened to a preselected depth, the surface region characterized by the formation of intragranular iron nitride particles and a substantial absence of an intergranular white phase, comprising the steps of:
Dependencies are inferred from the claim text.