Inert dental glass
Assignee3M Espe AG
InventorsStefan Hoescheler, Markus Mikulla, Gabriele Rackelmann, Volker Bambach
Life of this patent
Estimating the term…
Abstract
The invention relates to the use of ions of weakly basic oxides as linking ions for polyacids in cements, preferably polyelectrolyte cements. Suitable ions comprise elements of the scandium series, for example, Sc3+, Y3+, La3+, Ce4+ and all subsequent tri- and tetra-valent lanthanides and the ions Mg2+, Zn2+, Ga2+, In2+. The application of said ions permits a regulation of the cement reaction without surface treatment of the glass powder.
Claims20
A dental material comprising a dental glass characterized by the following composition:
- 7 Oxide Proportion Y2O3 + La2O3 + other lanthanide oxides 30 to 80% by weight B2O3 + Al2O3 + Ga2O3 5 to 50% by weight SiO2 + GeO2 + SnO 10 to 50% by weight P2O5 0 to 18% by weight MgO + CaO + SrO + ZnO + BaO + Li2O + 0 to 10% by weight Na2O + K2O + Rb2O + Cs2O TiO2 + ZrO2 + HfO2 0 to 10% by weight V2O5 + Nb2O5 + Ta2O5 0 to 10% by weight
- in which instead of the Y2O3+La2O3+other lanthanide oxides it is also possible for Sc2O3 to be present in an amount of from 20 to 50% by weight.
The dental material as claimed in one of the preceding claims, in which the glass is essentially a three-component system.
The dental material as claimed in one of the preceding claims, in which from 0 to 25% by weight of the oxygen in the dental glass is replaced by fluorine.
The dental material as claimed in one of the preceding claims, in which the dental glass is present in powder form with a specific BET surface area of 1 to 15 m2/g.
The dental material as claimed in one of the preceding claims, in which the dental glass has a mean grain size in the range from 0.01 to 10 μm.
The dental material as claimed in one of the preceding claims, in which the surface of the dental glass has not been surface-treated, for example by washing with acid, surface coating and/or conditioning, in order to adjust the setting time.
A process for producing a dental glass as described in one of the preceding claims, comprising the steps a) providing the oxidic substances, b) mixing the oxidic substances, c) melting the mixture from step b), d) quenching the molten material to form a solid, e) milling the solid from step d) to form a glass powder, the glass powder from step d) not being treated with acid before it is used in a dental cement.
The use of a dental glass as described in one of the preceding claims for production of a cement, without the surface of the glass having being surface-treated.
The use of ions of weakly basic-reacting oxides in glasses, which can enter into a cement reaction with a polyacid, to crosslink the polyacid.