Sol-gel derived porous microcomposite of perfluorinated ion-exchange polymer and metal oxide
AssigneeE. I. Du Pont de Nemours and Company
InventorsMark Andrew Harmer, Qun Sun
Life of this patent
Estimating the term…
Abstract
Porous microcomposites have been prepared from perfluorinated ion-exchange polymer and metal oxides such as silica using the sol-gel process. Such microcomposites possess high surface area and exhibit extremely high catalytic activity.
Claims56
A porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
The process of preparation of a porous microcomposite which comprises perfluorinated ion-exchange polymer containing pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm;
- said process comprising the steps of:
- a. mixing the perfluorinated ion-exchange polymer with one or more metal oxide precursors in a common solvent;
- b. initiating gelation;
- c. allowing sufficient time for gelation and aging of the mixture;
- and
- d. removing the solvent.
An improved process for the nitration of an aromatic compound wherein the improvement comprises contacting said aromatic compound with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
An improved process for the esterification of a carboxylic acid with an olefin wherein the improvement comprises contacting said carboxylic acid with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
A process for regenerating a catalyst comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 1 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm, comprising the steps of:
- (a) contacting the microcomposite with an acid;
- and
- (b) removing the excess acid to yield the regenerated catalyst.
An improved process for the dimerization of an alpha substituted styrene wherein the improvement comprises contacting said alpha substituted sytrene with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 1 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
An improved process for the alkylation of an aromatic compound with an olefin wherein the improvement comprises contacting said aromatic compound with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 1 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
An improved process for the polymerization of tetrahydrofuran to polytetramethylene ether acetate wherein the improvement comprises contacting said tetrahydrofuran with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
An improved process for the acylation of an aromatic compound with an acyl halide wherein the improvement comprises contacting said aromatic compound with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
A process for the isomerization of an olefin, comprising contacting said olefin at isomerization conditions with a catalytic amount of a porous microcomposite, said microcomposite comprising a perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.
Dependencies are inferred from the claim text.