Barrier film and laminated material, container for wrapping and image display medium using the same, and manufacturing method for barrier film
OwnerMinoru Komadainventor
Life of this patent
Estimating the term…
Loading patent…
OwnerMinoru Komadainventor
Estimating the term…
An object of the present invention is to provide a barrier film having the extremely high barrier property and the better transparency, a method for manufacturing the same, and a laminated material, a container for wrapping and an image displaying medium using the barrier film. According to the present invention, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, wherein the barrier layer is a silicon oxide film having an atomic ratio in a range of Si:O:C=100:160 to 190:30 to 50, a peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1030 to 1060 cm−1, a film density in a range of 2.5 to 2.7 g/cm3, and a distance between grains of 30 nm or shorter. Still more, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, wherein the barrier layer is a silicon oxi-nitride film having an atomic ratio in a range of Si:O:N:C=100:80 to 110:40 to 70:30 to 50, a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si-N stretching vibration in a range of 900 to 1000 cm−1, a film density in a range of 2.7 to 3.0 g/cm3, and a distance between grains of 30 nm or shorter.
A barrier film provided with a barrier layer on at least one surface of a substrate film, wherein
A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxide film having an atomic ratio in a range of Si:O:C=100:160 to 190:30 to 50, a peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1030 to 1060 cm−1, a film density in a range of 2.5 to 2.7 g/cm3 and a distance between grains of 30 nm or shorter, on a substrate film, using either of silicon having a sintered density of 80% or higher or SiOx (‘x’ is 1 to 2) having a sintered density of 80% or higher as a film forming material, in the presence of an oxygen gas by an ion plating method.
A barrier film provided with a barrier layer on at least one surface of a substrate film, wherein
A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxi-nitride film having an atomic ratio in a range of Si:O:N:C=100:80 to 110:40 to 70:30 to 50, a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si—N stretching vibration in a range of 900 to 1000 cm−1, a film density in a range of 2.7 to 3.0 g/cm3 and a distance between grains of 30 nm or shorter, on a substrate film, using either of silicon having a sintered density of 80% or higher or silicon oxide having a sintered density of 80% or higher as a film forming material, in the presence of a nitrogen gas, or in the presence of a nitrogen gas and an oxygen gas by an ion plating method.
Dependencies are inferred from the claim text.