Back to results
US 2003/0083455 A1Published application
Room temperature curable organopolysiloxane compositions
AssigneeShin-Etsu Chemical Co., Ltd.
InventorsJun Horikoshi, Tsuneo Kimura, Hironao Fujiki
Life of this patent
Estimating the term…
Abstract
A room temperature curable organopolysiloxane composition comprising (a) an organopolysiloxane having a specific structure, (b) a alkenoxysilane or substituted alkenoxysilane or a partial hydrolyzate thereof, and (c) a siloxane or a partial hydrolyzate thereof cures into a product which experiences no decline of insulation resistance upon application of voltage in a hot humid environment and is resistant to electrolytic corrosion.
Claims3
A room temperature curable organopolysiloxane composition comprising
- (a) 100 parts by weight of an organopolysiloxane having the following general formula (I):
- 12
- wherein R1 is hydrogen, a substituted or unsubstituted alkyl radical or a substituted or unsubstituted alkenyl radical, R2 is independently a substituted or unsubstituted monovalent hydrocarbon radical, X is an oxygen atom or a divalent hydrocarbon radical, a is 0, 1 or 2, and n is an integer of at least 10,
- (b) 1 to 30 parts by weight of a substituted or unsubstituted alkenoxysilane having the following general formula (II):
- 13
- wherein R3 is a substituted or unsubstituted monovalent hydrocarbon radical, R4 and R5 are each independently hydrogen or a substituted or unsubstituted monovalent hydrocarbon radical, and x is 3 or 4, or a partial hydrolyzate thereof, and
- (c) 0.01 to 10 parts by weight of a siloxane containing per molecule at least one monovalent radical having the general formula (III):
- 14
- wherein R6, R7, R8 and R9 each are hydrogen or a monovalent hydrocarbon radical, and y is an integer of 1 to 6, at least two silicon atoms, and at least three radicals selected from the group consisting of alkyl, alkoxy and alkenoxy radicals, or a partial hydrolyzate thereof.
6 more elements
Dependencies are inferred from the claim text.