Polybutylene terephthalate resin and compositions and molded articles comprising the resin
AssigneeMitsubishi Engineering-Plastics Corporation
InventorsKunihiro Takenaka, Ryo Saito, Hidekazu Shoji
Life of this patent
Estimating the term…
Loading patent…
AssigneeMitsubishi Engineering-Plastics Corporation
InventorsKunihiro Takenaka, Ryo Saito, Hidekazu Shoji
Estimating the term…
A polybutylene terephthalate resin having 30 eq/t or less of carboxyl end group, a crystallization temperature in a temperature decrease of 175° C. or higher and an amount of residual tetrahydrofuran of 300 ppm by weight or less; and compositions and molded articles comprising the resin and glass fiber, antioxidants and mold-releasing agents is provided. The polybutylene terephthalate resin can be molded in a short molding cycle, exhibits excellent resistance to hydrolysis and mold-releasing property, causes no corrosion of metals and generates little gas during molding. The compositions and the molded articles exhibit improved impact resistance, stability under heating and oxidation and mold-releasing property and can be advantageously used for members in electric and electronic products and in automobiles.
A polybutylene terephthalate resin having 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min.
A polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the resin.
A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min, and glass fiber.
A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin, and glass fiber.
A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min, and phenolic antioxidants.
A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin, and phenolic antioxidants.
A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has 30 eq/t or less of carboxyl end group and a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min, and a fatty acid ester which has a residue group of a fatty acid having 12 to 36 carbon atoms and a residue group of an alcohol having 1 to 36 carbon atoms.
A polybutylene terephthalate resin composition which comprises a polybutylene terephthalate resin which has a crystallization temperature in a temperature decrease of 175° C. or higher as measured by a differential scanning calorimeter at a rate of the temperature decrease of 20° C./min and an amount of residual tetrahydrofuran of 300 ppm by weight or less in the polybutylene terephthalate resin, and a fatty acid ester which has a residue group of a fatty acid having 12 to 36 carbon atoms and a residue group of an alcohol having 1 to 36 carbon atoms.
Dependencies are inferred from the claim text.